MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Dow ENGAGE™ 7387 EL Polyolefin
Categories: Polymer; Thermoplastic; Polyolefin

Material Notes: Product Description: ENGAGE™ 7387 EL Polyolefin Elastomer is a revolutionary butane copolymer with higher molecular weight, better toughness, and higher melt strength than other commercially available polyolefin elastomers. It is well suited for extruded applications such as Wire & Cable.
Main Characteristics:
  • Pellet form
  • High melt strength
  • Improved toughness
  • Talc dusted (untreated, 1 µm)
Applications:
  • Wire & Cable
Availability: Asia Pacific; Europe; North America

Uses: Blending; Compounding; Medium Voltage Insulation; Wire & Cable Applications

Agency Ratings: EU No 10/2011

Form: Pellets

Information provided by The Dow Chemical Company

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.872 g/ccASTM D792
Mooney Viscosity 51
@Temperature 121 °C
ML1+4; ASTM D1646
Melt Flow <= 0.50 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 74Compression Molded; ASTM D2240
Hardness, Shore D 22Compression Molded; ASTM D2240
Tensile Strength at Break 754 psiCompression Molded, 20 in/min; ASTM D638
Elongation at Break 500 %Compression Molded, 20 in/min; ASTM D638
Tensile Modulus 377 psi100% Secant, 20 in/min, Compression Molded; ASTM D638
Flexural Modulus 1580 psi2% Secant, Compression Molded; ASTM D790
 1640 psi1% Secant, Compression Molded; ASTM D790
Tear Strength 217 pliDie C; ASTM D624
 
Thermal PropertiesOriginal ValueComments
Melting Point 124 °F
Crystallization Temperature 98.6 °FPeak
Vicat Softening Point 117 °FASTM D1525
Glass Transition Temp, Tg -61.6 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PDOWF514 / 311207

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.