MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

CRP  Windform

(Viewing data as-entered. Click here to return)
BASF 3D Ultrafuse® TPU 85A Fused Fillament
Categories: Polymer; 3D Printing/Additive Manufacturing Polymer; Thermoplastic; Polyurethane, TP

Material Notes: Components: BASF ether based thermoplastic polyurethane (TPU) based filament for Fused Filament Fabrication.

Product Description: Ultrafuse® TPU 85A comes in its natural white color. Chemical properties (e.g. resistance against particular substances) and tolerance for solvents can be made available, if these factors are relevant for a specific application. Generally, these properties correspond to publicly available data on polyether based TPUs. This material is not FDA conform. Good flexibility at low temperature, good wear performance and good damping behavior are the key features of Ultrafuse® TPU 85A.

Information provided by BASF

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.111 g/ccPrinted Part; ISO 1183-1
Melt Flow 11.8877 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ISO 1133
Storage Temperature 15.0 - 25.0 °C
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 85
@Time 3.00 sec
ISO 7619-1
Hardness, Shore D 29
@Time 15.0 sec
ISO 7619-1
Tensile Strength at Break 10.0 MPaZX: Upright; ISO 527
 34.0 MPaXY: Flat; ISO 527
Tensile Stress 6.20 MPa
@Strain 50 %
ZX: Upright; ISO 527
 7.20 MPa
@Strain 50 %
XY: Flat; ISO 527
 7.50 MPa
@Strain 100 %
ZX: Upright; ISO 527
 8.70 MPa
@Strain 100 %
XY: Flat; ISO 527
 9.00 MPa
@Strain 200 %
ZX: Upright; ISO 527
 10.1 MPa
@Strain 200 %
XY: Flat; ISO 527
Elongation at Break 320 %ZX: Upright; ISO 527
 600 %XY: Flat; ISO 527
Modulus of Elasticity 20.0 GPaYoung's, XY: Flat; ISO 527
 27.0 GPaYoung's, ZX: Upright; ISO 527
Izod Impact, Notched (ISO) NBXY: Flat; ISO 180
 NBXZ: On its edge; ISO 180
 NBZX: Upright; ISO 180
Charpy Impact Unnotched NB
@Time -108000 sec
XY: Flat; ISO 179-2
 NB
@Time -108000 sec
XZ: On its edge; ISO 179-2
 NB
@Time -108000 sec
ZX: Upright; ISO 179-2
Charpy Impact, Notched NBXY: Flat; ISO 179-2
 NBXZ: On its edge; ISO 179-2
 NBZX: Upright; ISO 179-2
 9.30 kJ/m²
@Time -108000 sec
ZX: Upright; ISO 179-2
 47.3 kJ/m²
@Time -108000 sec
XY: Flat; ISO 179-2
 95.4 kJ/m²
@Time -108000 sec
XZ: On its edge; ISO 179-2
Tensile Impact Strength 111 kJ/m²ZX: Upright; ISO 8256-1
 NBXY: Flat; ISO 8256-1
 NBXZ: On its edge; ISO 8256-1
Tear Strength 18.0 kN/mXZ: On its edge; ISO 34-1
 30.0 kN/mZX: Upright; ISO 34-1
 80.0 kN/mXY: Flat; ISO 34-1
Abrasion 82mm3; ISO 4649
Compression Set 26 %
@Temperature 23.0 °C,
Time 259000 sec
ISO 815-1
 52 %
@Temperature 70.0 °C,
Time 86400 sec
ISO 815-1
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 2.10e+11 ohm-cmZX: Upright; IEC 62631-3-1
 2.60e+11 ohm-cmXY: Flat; IEC 62631-3-1
Dielectric Strength 17.0 kV/mmZX: Upright; IEC 60243-1
 21.0 kV/mmXY: Flat; IEC 60243-1
 
Thermal PropertiesOriginal ValueComments
Glass Transition Temp, Tg -44.0 °CISO 11357-2
 
Processing PropertiesOriginal ValueComments
Processing Temperature 40.0 °CBed, Bed Material: Glass
Nozzle Temperature 200 - 220 °C
Drying Temperature 70.0 °Cin a hot air dryer or vacuum oven
Dry Time 5.00 hour
Shelf Life 12.0 Month
 
Descriptive Properties
Nozzle Diameter=0.4 mm
Print speed15-40 mm/s

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PBASF3D026 / 312267

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.