MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
Kolon CD901 Industrial Film  (discontinued **)
Categories: Polymer; Film

Material Notes: Excellent clarity makes an ideal support material for various coated films. CD Series grades are often selected as a component of a printed & laminated package because of great tensile strength, high temperature resistance, gas barrier property, and chemical resistance.

Uses: Graphic Printing, Spacer Tape, Carrier, Membrane Switch, Frame, Tape, Release, Label, Window, Spangle, Laminex, Deco, Adhesive Tape, PU Sheet Form, Coating Purposes, Furniture

Information provided by Kolon

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Thickness 50.0 - 250 microns
Surface Tension 52 dynes/cmInside; ASTM D2578
 
Mechanical PropertiesOriginal ValueComments
Film Elongation at Break, MD 210 %
@Thickness 0.0750 mm
ASTM D882
 230 %
@Thickness 0.100 mm
ASTM D882
 240 %
@Thickness 0.125 mm
ASTM D882
Film Elongation at Break, TD 120 %
@Thickness 0.0750 mm
ASTM D882
 130 %
@Thickness 0.100 mm
ASTM D882
 180 %
@Thickness 0.125 mm
ASTM D882
Coefficient of Friction, Dynamic 0.35
@Thickness 0.0750 mm
ASTM D1894
 0.35
@Thickness 0.100 mm
ASTM D1894
 0.35
@Thickness 0.125 mm
ASTM D1894
Coefficient of Friction, Static 0.30
@Thickness 0.0750 mm
ASTM D1894
 0.30
@Thickness 0.100 mm
ASTM D1894
 0.30
@Thickness 0.125 mm
ASTM D1894
Film Tensile Strength at Break, MD 176 MPa
@Thickness 0.100 mm
ASTM D882
 176 MPa
@Thickness 0.125 mm
ASTM D882
 186 MPa
@Thickness 0.0750 mm
ASTM D882
Film Tensile Strength at Break, TD 167 MPa
@Thickness 0.125 mm
ASTM D882
 186 MPa
@Thickness 0.100 mm
ASTM D882
 206 MPa
@Thickness 0.0750 mm
ASTM D882
 
Thermal PropertiesOriginal ValueComments
Shrinkage, MD 1.0 %
@Thickness 0.0750 mm
Heat Shrinkage; ASTM D2305
 1.0 %
@Thickness 0.100 mm
Heat Shrinkage; ASTM D2305
 1.0 %
@Thickness 0.125 mm
Heat Shrinkage; ASTM D2305
Shrinkage, TD 0.00 %
@Thickness 0.0750 mm
Heat Shrinkage; ASTM D2305
 0.20 %
@Thickness 0.100 mm
Heat Shrinkage; ASTM D2305
 0.20 %
@Thickness 0.125 mm
Heat Shrinkage; ASTM D2305
 
Optical PropertiesOriginal ValueComments
Haze 1.3 %
@Thickness 0.0750 mm
ASTM D1003
 1.5 %
@Thickness 0.100 mm
ASTM D1003
 2.3 %
@Thickness 0.125 mm
ASTM D1003

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Covestro Platilon® M2234 Polyether-Blockamide Film
Precision Polymer Engineering Q90A Polyurethane Rubber
Precision Polymer Engineering Q90Y Polyurethane Rubber
Precision Polymer Engineering Q70Y Polyurethane Rubber
Precision Polymer Engineering Q70X Polyurethane Rubber

PKOKZ815 / 185358

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.