MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Titanium Grade 1, Annealed
Categories: Metal; Nonferrous Metal; Titanium Alloy; Unalloyed/Modified Titanium

Material Notes: Information provided by Allvac and the references.

Applications: Airframe components, cryogenic vessels, heat exchangers, CPI equipment, condenser tubing, pickling baskets. Sample was annealed 2 hr at 700°C..

Forms typically available: billet, bar, plate, sheet, strip, rod, wire, extrusions, tubing.

Titanium Grades 1,2,3,4,7,11,and 12 are all considered unalloyed and have similar mechanical properties.

Key Words: UNS R50250; ASTM Grade 1, CP titanium, C.P. titanium alloy
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 4.51 g/cc
 
Mechanical PropertiesOriginal ValueComments
Hardness, Brinell 120
Hardness, Knoop 132Estimated from Brinell.
Hardness, Rockwell B 90
Hardness, Vickers 122Estimated from Brinell.
Tensile Strength 152 MPa
@Temperature 316 °C
Tensile Strength, Ultimate 330 MPa
Tensile Strength, Yield 240 MPa
Elongation at Break 30 %
Tensile Modulus 100 GPa
Modulus of Rigidity 38.6 GPa
Compressive Yield Strength 340 MPa
Poissons Ratio 0.34
Shear Modulus 38.0 GPa
Charpy Impact 140 JV-notch
Bend Radius, Minimum 2.0 t
@Thickness >=1.80 mm
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.0000450 ohm-cm
 
Thermal PropertiesOriginal ValueComments
Heat of Fusion 325 J/gHigh Purity Ti.
CTE, linear 8.35 µm/m-°C
@Temperature 15.0 °C
 8.60 µm/m-°C
@Temperature 20.0 - 93.0 °C
 9.20 µm/m-°C
@Temperature 200 °C
 19.9 µm/m-°C
@Temperature 20.0 °C
perpendicular
Specific Heat Capacity 0.520 J/g-°C
 0.560 J/g-°C
@Temperature 200 °C
 0.620 J/g-°C
@Temperature 400 °C
 0.690 J/g-°C
@Temperature 600 °C
Thermal Conductivity 16.0 W/m-K
Melting Point <= 1670 °C
Liquidus 1670 °C
Beta Transus 888 °C
 
Optical PropertiesOriginal ValueComments
Emissivity (0-1) 0.30
@Temperature 710 °C
High purity Ti
Reflection Coefficient, Visible (0-1) 0.56High purity Ti; visible light.
 
Component Elements PropertiesOriginal ValueComments
Carbon, C <= 0.10 %
Hydrogen, H <= 0.015 %
Iron, Fe <= 0.20 %
Nitrogen, N <= 0.030 %
Other, total <= 0.30 %
Oxygen, O <= 0.18 %
Titanium, Ti 99.5 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Titanium Grade 1
Titanium Grade 2, Annealed
Titanium Grade 2
TIMET TIMETAL® 35A CP Titanium (ASTM Grade 1)
Titanium Grade 4

MTU011 / 14258

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.