Hostacom ERC 204N D is an 10% talc filled PP copolymer, with high stiffness, low filler content and good scratch resistance. Advanced technologies allowed for a significant reduction of mineral filler which contributed to the reduction of final part weight. This grade is delivered in customer customized colors, some properties may be slightly altered upon color selected. Applications: Automotive Parts, Interior Automotive Applications, Interior TrimsInformation provided by LyondellBasell. |