MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
KaMin Nucote® 7009 Kaolin Clay - Surface Treated
Categories: Ceramic; Clay; Kaolin Clay

Material Notes: Organophilic kaolin clay for use in producing low foaming slab-dips and pellet lubricants.

Industry: Rubber & Plastic

Uses: Mold Release

Information provided by KaMin LLC.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 2.60 g/cc
Moisture Absorption at Equilibrium <= 2 %As Produced
Particle Size 0.30 µmAverage Stokes Equivalent Diameter
Particle Mesh Size 325 Mesh0.2% Retained
pH 7100 g/250 ml H2O Slurry
 
Descriptive Properties
CAS Number1332-58-7
Crystalline Silica (quartz)<0.1%
Physical FormDry
Shipping PointMacon, GA

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Alcoa 7055-T77511 Aluminum Extrusions
7009 Aluminum Composition Spec
Illite KAl2(AlSi3O10)-(OH)2
Fainplast Compounds GS 7009 Flexible PVC, Injection Molding for Footwear
BCC Products BC 7009-2 Epoxy Casting

CKAMAN933 / 178404

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.