N,N` Ethylene Bis-stearamide STRUKTOL® TR EBS is an exceptionally effective dispersion aid for a wide range of organic and inorganic pigments. STRUKTOL® TR EBS can be used in most polymer carrier systems. FDA Status: 175.105; 175.300; 176.170; 176.180; 177.1200; 177.1350; 177.1400; 177.2470; 177.2480 |