MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
3M AC-350 Class C-1/2 Aerospace Sealant
Categories: Polymer; Thermoset; Polysulfide Sealant/Adhesive

Material Notes: 3M Aerospace Sealant AC-350 Class C are fast-cure, intermediate density polysulfide sealant suitable fro fuel tank and fuselage applications. These two-component, manganese dioxide cured sealant have resistance to aviation gasoline and jet fuel, as well as resistance to chemicals and petroleum products common to other aircraft industry. 3M AC-350 Class C Sealants maintain flexibility and bond strength on most metal substrates such as aluminum, titanium, steel, stainless steel, and many coatings under extremes of temperature, weathering and stress. The mixed compound is a flowable, faying surface grade material easily applied by brush, roller, spatula, or extrusion gun. The sealant exhibits good tooling properties.

Information provided by 3M

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density <= 1.40 g/cccured 14 days @ 50% RH
Volatiles 5.0 %
Brookfield Viscosity 200000 - 350000 cPBase, RVF #7 sp @ 2 rpm
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 50 - 55cured 14 days @ 50% RH
Shear Strength 240 psi
@Time 1.21e+6 sec
Graphite Bismaleimide (BMI) composite IM7/5250-4
 270 psi
@Time 346000 sec
AMS4911 Titanium
Peel Strength 37.0 pli
@Temperature 60.0 °C,
Time 605000 sec
in JRF, Graphite/BMI
 38.0 pli
@Temperature 60.0 °C,
Time 605000 sec
in JRF, MIL-C-27725
 39.0 pli
@Temperature 60.0 °C,
Time 605000 sec
in JRF/SW, Graphite/BMI
 41.0 pli
@Temperature 60.0 °C,
Time 605000 sec
in JRF, MIL-C-5541
 42.0 pli
@Temperature 60.0 °C,
Time 605000 sec
in JRF/SW, MIL-C-27725
 42.0 pli
@Temperature 60.0 °C,
Time 605000 sec
in JRF/SW, MIL-PRF-85582
 45.0 pli
@Temperature 60.0 °C,
Time 605000 sec
in JRF/SW, MIL-C-5541
 45.0 pli
@Temperature 60.0 °C,
Time 605000 sec
in JRF, AMS 4911 Titanium
 45.0 pli
@Temperature 60.0 °C,
Time 6.05e+6 sec
in JRF/SW, AMS 4911 Titanium
 45.0 pli
@Temperature 60.0 °C,
Time 605000 sec
in JRF, MIL-PRF-85582
 47.0 pli
@Temperature 60.0 °C,
Time 605000 sec
in JRF/SW, AMS 4911 Titanium
 57.0 pli
@Temperature 60.0 °C,
Time 6.05e+6 sec
in JRF, AMS 4911 Titanium
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 121 °Ccured 14 days @ 50% RH
 182 °CShort term, cured 14 days @ 50% RH
Minimum Service Temperature, Air -54.0 °Ccured 14 days @ 50% RH
 
Processing PropertiesOriginal ValueComments
Cure Time 2.00 - 3.00 hour
Tack-Free Time 2.00 - 3.00 hour
Shelf Life 9.00 Month
@Temperature <=26.7 °C
 
Descriptive Properties
AppearanceBrownAccelerator
 Dark Gray
 Off WhiteBase

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Evonik Compimide® TM123 4,4'-Bis(o-propenylphenoxy)benzophenone
Hexcel® HexPly® F650 Bismaleimide Resin
Hexcel® HexFlow® RTM651 One-part Modified BMI Resin
Henkel Hysol EA 9833.1 (BMI) Core Splice Adhesive
Henkel Hysol EA 9673 (BMI) Film Adhesive

PMM35390 / 170137

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.