MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Hapco Ultraclear™ 480N-10 Two Component Polyurethane
Categories: Polymer; Thermoset; Polyurethane, TS

Material Notes: Ultraclear™ is new series of diamond clear casting resins that are UV resistant, have high physical properties, and are available in multiple gel times. Ultraclear™ can be used in a wide variety of applications that require exceptional clarity; e.g., encapsulation, optical components, test models, and display pieces. The range of gel times makes Ultraclear™ suitable for small, average sized or larger castings.

KEY ADVANTAGES:

  • Diamond Clear
  • UV Resistant
  • Mercury Free
  • 1:1 Mix Ratio
  • Low Viscosity
  • High Impact Resistance

Information provided by Hapco, Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.08 g/ccASTM D-4669
Viscosity 600 cPASTM D-4878
Linear Mold Shrinkage 0.0020 - 0.0060 in/inASTM D-2566
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 80ASTM D-2240
Tensile Strength 7700 psiASTM D-638
Elongation at Break 13 %ASTM D-638
Modulus of Elasticity 338 ksiASTM D-638
Flexural Strength 11400 psiASTM D-790
Flexural Modulus 318 ksiASTM D-790
Izod Impact, Notched 1.10 ft-lb/inASTM D-256
Izod Impact, Unnotched >= 17.1 ft-lb/inASTM D-256
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 76.0 °CASTM D-648
Deflection Temperature at 1.8 MPa (264 psi) 70.0 °CASTM D-648
 
Optical PropertiesOriginal ValueComments
Refractive Index 1.585ASTM D-542
 
Processing PropertiesOriginal ValueComments
Cure Time 5.00 - 8.00 hour
@Thickness 3.17 mm
Demold
 1.00 - 2.00 hour
@Thickness 3.17 mm,
Temperature 26.7 °C
Demold
Gel Time 10.0 min
@Load 0.100 kg
ASTM D-2971
 
Descriptive Properties
Color (cured)Water Clear
Mix Ratio100:100Volume
 100:100Weight

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PHAPCO174 / 317233

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.