MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
SABIC NORYL GTX™ Resin GTX914 Polyphenylene Ether + PA (PPE+Nylon) (Americas)
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Polyphenylene Ether/PPO

Material Notes: NORYL GTX™ 914 resin is a non-reinforced alloy of Polyphenylene Ether (PPE) + Polyamide (PA). This injection moldable grade exhibits an ideal combination of impact performance and dimensional stability at elevated temperatures along with excellent chemical resistance and processability. NORYL GTX914 resin may be an excellent candidate for various automotive applications such as tank flaps, exterior trim, and wheel covers.

Features: Hydrolytic Stability,Chemical Resistance,Low Creep Sensitivity,Good Stiffness,Low Warpage,High Impact Resistance

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.10 g/ccASTM D792
Density 1.09 g/ccISO 1183
Moisture Absorption 0.0700 %Injection Molding
 1.20 %23°C / 50% RH; ISO 62
Water Absorption at Saturation 3.5 %ISO 62-1
Viscosity 11 cP
@Load 5.00 kg,
Temperature 280 °C
MVR cc/10 min; ISO 1133
Linear Mold Shrinkage, Flow 0.015 - 0.019 cm/cmSABIC method
 0.013 - 0.016 cm/cm
@Thickness 3.20 mm
SABIC method
Linear Mold Shrinkage, Transverse 0.011 - 0.014 cm/cm
@Thickness 3.20 mm
SABIC method
Melt Flow 12 g/10 min
@Load 5.00 kg,
Temperature 280 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Ball Indentation Hardness 90.0 MPaH358/30; ISO 2039-1
Tensile Strength at Break 55.0 MPa50 mm/min; ASTM D638
 55.0 MPa50 mm/min; ISO 527
Tensile Strength, Yield 55.0 MPa50 mm/min; ASTM D638
 55.0 MPa50 mm/min; ISO 527
Elongation at Break 60 %50 mm/min; ISO 527
 100 %50 mm/min; ASTM D638
Elongation at Yield 7.5 %50 mm/min; ISO 527
 15 %50 mm/min; ASTM D638
Tensile Modulus 1950 MPa50 mm/min; ASTM D638
 2100 MPa1 mm/min; ISO 527
Flexural Strength 80.0 MPayield, 2 mm/min; ISO 178
 80.0 MPayld, 1.3 mm/min, 50 mm span; ASTM D790
Flexural Modulus 1900 MPa1.3 mm/min, 50 mm span; ASTM D790
 2000 MPa2 mm/min; ISO 178
Izod Impact Notched 280 JASTM D256
 120 J
@Temperature -30.0 °C
ASTM D256
Izod Impact, Notched (ISO) 30.0 kJ/m²80*10*4; ISO 180/1A
 15.0 kJ/m²
@Temperature -30.0 °C
80*10*4; ISO 180/1A
Charpy Impact, Notched 30.0 kJ/m²ISO 179/2C
 30.0 kJ/m²Edgew 80*10*4 sp=62mm; ISO 179/1eA
 15.0 kJ/m²
@Temperature -30.0 °C
Edgew 80*10*4 sp=62mm; ISO 179/1eA
Dart Drop, Total Energy 60.0 JASTM D3763
Taber Abrasion, mg/1000 Cycles 15CS-17, 1 kg; SABIC method
 
Electrical PropertiesOriginal ValueComments
Dielectric Constant 2.7
@Frequency 1e+6 Hz
IEC 60250
 3.5
@Frequency 50.0 - 60.0 Hz
IEC 60250
Dielectric Strength 20.0 kV/mm
@Thickness 3.20 mm
in oil; IEC 60243-1
Dissipation Factor 0.024
@Frequency 1e+6 Hz
IEC 60250
 0.072
@Frequency 50.0 - 60.0 Hz
IEC 60250
Comparative Tracking Index 600 VIEC 60112
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 90.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
ASTM E831
 90.0 µm/m-°C
@Temperature 23.0 - 60.0 °C
ISO 11359-2
CTE, linear, Transverse to Flow 90.0 µm/m-°C
@Temperature 23.0 - 60.0 °C
ISO 11359-2
 95.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
ASTM E831
Thermal Conductivity 0.230 W/m-KISO 8302
Hot Ball Pressure Test 125 °CPASS; IEC 60695-10-2
Deflection Temperature at 0.46 MPa (66 psi) 180 °CEdgew 120*10*4 sp=100mm; ISO 75/Be
 180 °C
@Thickness 3.20 mm
unannealed; ASTM D648
Vicat Softening Point 190 °CRate B/50; ISO 306
 195 °CRate B/50; ASTM D1525
 195 °CRate B/120; ISO 306
 245 °CRate A/50; ISO 306
Flammability, UL94 HB
@Thickness 1.60 mm
UL 94 by SABIC-IP
 
Processing PropertiesOriginal ValueComments
Nozzle Temperature 270 - 300 °C
Zone 2 270 - 290 °C
Zone 3 280 - 300 °C
Melt Temperature 280 - 310 °CInjection Molding
Mold Temperature 80.0 - 120 °C
Drying Temperature 100 - 120 °CInjection Molding
Dry Time 2.00 - 3.00 hourInjection Molding
Precipitation Temperature 60.0 - 80.0 °CHopper Temperature

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSABH82162 / 290109

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.