MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
Overview of materials for Epoxy Molding Compound
Categories: Polymer; Thermoset; Epoxy; Epoxy Molding Compound

Material Notes: This property data is a summary of similar materials in the MatWeb database for the category "Epoxy Molding Compound". Each property range of values reported is minimum and maximum values of appropriate MatWeb entries. The comments report the average value, and number of data points used to calculate the average. The values are not necessarily typical of any specific grade, especially less common values and those that can be most affected by additives or processing methods.

Vendors: Master Bond is a leading manufacturer of high performance epoxy adhesives, sealants, coatings, potting/encapsulation compounds and impregnation resins. Our epoxies include one and two part formulations that can be cured at room temperature, with heat or exposure to UV light. Special formulations feature high electrical and/or thermal conductivity and wide service temperature ranges. Visit www.masterbond.com.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Density 0.550 - 2.45 g/ccAverage value: 1.78 g/cc Grade Count:100
Water Absorption 0.00340 - 0.900 %Average value: 0.180 % Grade Count:43
Moisture Absorption at Equilibrium 0.230 - 0.600 %Average value: 0.363 % Grade Count:12
Viscosity 600 - 45000 cP
@Temperature 165 - 175 °C
Average value: 6480 cP Grade Count:48
 1700 - 1700 cP
@Temperature 175 - 175 °C
Average value: 6480 cP Grade Count:1
 1700 - 1700 cP
@Diameter 0.500 - 0.500 mm
Average value: 6480 cP Grade Count:1
Linear Mold Shrinkage 0.0000900 - 0.00700 cm/cmAverage value: 0.00257 cm/cm Grade Count:63
Spiral Flow 48.0 - 180 cmAverage value: 107 cm Grade Count:52
Ash 71.4 - 88.6 %Average value: 79.3 % Grade Count:37
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell M 85.0 - 105Average value: 98.3 Grade Count:3
Hardness, Shore D 55.0 - 86.0Average value: 76.1 Grade Count:55
Tensile Strength, Ultimate 13.8 - 300 MPaAverage value: 85.2 MPa Grade Count:51
Elongation at Break 0.300 - 2.00 %Average value: 0.864 % Grade Count:11
Modulus of Elasticity 1.38 - 46.0 GPaAverage value: 17.3 GPa Grade Count:16
Flexural Yield Strength 35.5 - 400 MPaAverage value: 136 MPa Grade Count:99
 6.86442 - 58.8399 MPa
@Temperature 215 - 260 °C
Average value: 28.0 MPa Grade Count:26
Flexural Modulus 2.41 - 32.0 GPaAverage value: 16.3 GPa Grade Count:94
 0.686465 - 10.1008 GPa
@Temperature 215 - 260 °C
Average value: 4.23 GPa Grade Count:26
Compressive Yield Strength 6.89 - 350 MPaAverage value: 195 MPa Grade Count:48
Compressive Modulus 1.03 - 35.0 GPaAverage value: 8.95 GPa Grade Count:5
Adhesive Bond Strength 8.96 - 15.9 MPaAverage value: 11.7 MPa Grade Count:3
 13.8 - 15.9 MPa
@Temperature -55.0 - 93.0 °C
Average value: 14.9 MPa Grade Count:1
Izod Impact, Notched 0.160 - 21.0 J/cmAverage value: 3.06 J/cm Grade Count:31
Charpy Impact Unnotched 0.200 - 0.900 J/cm²Average value: 0.610 J/cm² Grade Count:5
Charpy Impact, Notched 0.150 - 8.00 J/cm²Average value: 3.30 J/cm² Grade Count:15
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 5080 - 5.60e+16 ohm-cmAverage value: 9.75e+15 ohm-cm Grade Count:46
 1.00e+9 - 3.20e+12 ohm-cm
@Temperature 150 - 150 °C
Average value: 1.03e+12 ohm-cm Grade Count:8
Surface Resistance 1.00e+12 - 1.00e+15 ohmAverage value: 2.31e+14 ohm Grade Count:5
Dielectric Constant 1.80 - 7.00Average value: 3.98 Grade Count:79
Dielectric Strength 1.40 - 55.1 kV/mmAverage value: 19.6 kV/mm Grade Count:83
Dissipation Factor 0.000300 - 0.0500Average value: 0.0115 Grade Count:68
Arc Resistance 120 - 240 secAverage value: 176 sec Grade Count:48
Comparative Tracking Index 200 - 600 VAverage value: 433 V Grade Count:13
 
Thermal PropertiesOriginal ValueComments
CTE, linear 3.30 - 80.0 µm/m-°CAverage value: 30.0 µm/m-°C Grade Count:79
 15.0 - 25.0 µm/m-°C
@Temperature 50.0 - 150 °C
Average value: 19.2 µm/m-°C Grade Count:3
CTE, linear, Transverse to Flow 27.0 - 80.0 µm/m-°CAverage value: 53.5 µm/m-°C Grade Count:29
Thermal Conductivity 0.400 - 3.60 W/m-KAverage value: 0.772 W/m-K Grade Count:57
Maximum Service Temperature, Air 93.0 - 250 °CAverage value: 178 °C Grade Count:6
Deflection Temperature at 1.8 MPa (264 psi) 122 - 282 °CAverage value: 248 °C Grade Count:31
Deflection Temperature at 8.0 MPa 115 - 180 °CAverage value: 145 °C Grade Count:5
Glass Transition Temp, Tg 75.0 - 228 °CAverage value: 174 °C Grade Count:64
Flammability, UL94 HB - V-0Grade Count:62
Oxygen Index 28.0 - 34.0 %Average value: 31.8 % Grade Count:18
 
Processing PropertiesOriginal ValueComments
Processing Temperature 135 - 193 °CAverage value: 172 °C Grade Count:18
Mold Temperature 160 - 190 °CAverage value: 175 °C Grade Count:39
Cycle Time - Injection 30.0 - 150 secAverage value: 82.0 sec Grade Count:5
Cure Time 0.250 - 10100 minAverage value: 489 min Grade Count:28
 0.000 - 720 min
@Temperature 65.0 - 177 °C
Average value: 131 min Grade Count:35
Pot Life 4.00 - 60.0 minAverage value: 25.0 min Grade Count:3

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Overview of materials for Epoxy Cure Resin
Overview of materials for Epoxy, Cast, Unreinforced
Overview of materials for Vinyl Ester Sheet Molding Compound
Overview of materials for Epoxy, Molded, Glass Fiber Filler
Overview of materials for Epoxy Adhesive

O1707 / 77892

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.