MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
DuPont Mobility and Materials Zytel® 8018HS NC010 PA66-IGF14  (discontinued **)
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, 10% Glass Fiber Filled

Material Notes: 14% Glass Reinforced, Toughened, Heat Stabilized, Polyamide 66

While this product line has been acquired by Celanese, this specific grade had been disconued while still a DuPont product so it is listed here as a discontinued DuPont product.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.19 g/ccDAM; ISO 1183
Water Absorption 6.3 %
@Thickness 2.00 mm
DAM; Sim. to ISO 62
Moisture Absorption 1.90 %
@Thickness 2.00 mm
DAM; Sim. to ISO 62
Linear Mold Shrinkage, Flow 0.0040 cm/cmDAM; ISO 294-4, 2577
Linear Mold Shrinkage, Transverse 0.0080 cm/cmDAM; ISO 294-4, 2577
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell M 70DAM; ISO 2039-2
Hardness, Rockwell R 110DAM; ISO 2039-2
Tensile Strength at Break 58.0 MPa50% RH; ISO 527-1/-2
 85.0 MPaDAM; ISO 527-1/-2
Elongation at Break 6.0 %DAM; ISO 527-1/-2
 14 %50% RH; ISO 527-1/-2
Tensile Modulus 2300 MPa50% RH; ISO 527-1/-2
 4200 MPaDAM; ISO 527-1/-2
Flexural Modulus 2000 MPa50% RH; ISO 178
 3600 MPaDAM; ISO 178
Poissons Ratio 0.36DAM; ISO 527-1/-2
 0.3950%RH; ISO 527-1/-2
Izod Impact, Notched (ISO) 70.0 kJ/m²
@Temperature -30.0 °C
50% RH; ISO 180/1U
 90.0 kJ/m²
@Temperature 23.0 °C
DAM; ISO 180/1U
 90.0 kJ/m²
@Temperature -30.0 °C
DAM; ISO 180/1U
 100 kJ/m²
@Temperature 23.0 °C
50% RH; ISO 180/1U
Izod Impact, Unnotched (ISO) 5.00 kJ/m²
@Temperature -30.0 °C
50% RH; ISO 180/1A
 5.00 kJ/m²
@Temperature -40.0 °C
50% RH; ISO 180/1A
 7.00 kJ/m²
@Temperature -40.0 °C
DAM; ISO 180/1A
 10.0 kJ/m²
@Temperature -30.0 °C
DAM; ISO 180/1A
 13.0 kJ/m²
@Temperature 23.0 °C
DAM; ISO 180/1A
 18.0 kJ/m²
@Temperature 23.0 °C
50% RH; ISO 180/1A
Charpy Impact Unnotched 75.0 kJ/m²
@Temperature -30.0 °C
50% RH; ISO 179/1eU
 80.0 kJ/m²
@Temperature 23.0 °C
DAM; ISO 179/1eU
 80.0 kJ/m²
@Temperature -30.0 °C
DAM; ISO 179/1eU
 100 kJ/m²
@Temperature 23.0 °C
50% RH; ISO 179/1eU
Charpy Impact, Notched 4.00 kJ/m²
@Temperature -40.0 °C
50% RH; ISO 179/1eA
 4.00 kJ/m²
@Temperature -40.0 °C
DAM; ISO 179/1eA
 6.00 kJ/m²
@Temperature -30.0 °C
50% RH; ISO 179/1eA
 6.00 kJ/m²
@Temperature -30.0 °C
DAM; ISO 179/1eA
 14.0 kJ/m²
@Temperature 23.0 °C
DAM; ISO 179/1eA
 18.0 kJ/m²
@Temperature 23.0 °C
50% RH; ISO 179/1eA
 
Electrical PropertiesOriginal ValueComments
Comparative Tracking Index 580 VDAM; IEC 60112
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 50.0 µm/m-°CDAM; ISO 11359-1/-2
CTE, linear, Transverse to Flow 118 µm/m-°CDAM; ISO 11359-1/-2
Melting Point 263 °C10°C/min; DAM; ISO 11357-1/-3
Deflection Temperature at 0.46 MPa (66 psi) 246 °CDAM; ISO 75-1/-2
Deflection Temperature at 1.8 MPa (264 psi) 195 °CDAM; ISO 75-1/-2
Flammability, UL94 HB
@Thickness 0.750 mm
DAM; IEC 60695-11-10
 HB
@Thickness 1.50 mm
DAM; IEC 60695-11-10
Flame Spread <= 80.0 mm/min
@Thickness 1.00 mm
ISO 3795 (FMVSS 302)
Oxygen Index 21 %DAM; ISO 4589-1/-2
 
Processing PropertiesOriginal ValueComments
Melt Temperature 285 - 305 °CInjection
 295 °CInjection Optimum
Mold Temperature 50.0 - 100 °CInjection
 80.0 °CInjection Optimum
Ejection Temperature 210 °CInjection
Drying Temperature 80.0 °CInjection
Dry Time 2.00 - 4.00 hourDehumidified Dryer; Injection
Moisture Content 0.20 %Injection
Hold Pressure 50.0 - 100 MPaInjection
 
Descriptive Properties
AdditivesRelease agent
Delivery formPellets
Drying RecommendedyesInjection
FMVSS ClassBISO 3795 (FMVSS 302)
Hold pressure time (s/mm)3Injection
Max. screw tangential speed (m/s)0.2Injection
Part Marking CodePA66-IGF14ISO 11469
ProcessingInjection Molding
Regional AvailabilityNorth America
 South and Central America
Resin IdentificationPA66-IGF14ISO 1043
Special characteristicsHeat stabilized or stable to heat

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Ascend Performance Materials Vydyne® R413H NT Impact Modified Nylon 66, Glass Filled
Ravago Manufacturing Americas Hylon® N1013HL Nylon 6/6 (Cond)
Celanese Zytel® 8018HS BKB085 PA66-IGF14
EMS-Grivory Grilon® BGZ-30/2 PA6-GF30
Ravago Manufacturing Americas Hylon® N1013THL Nylon 6/6 (DAM)

PDSX5375 / 198015

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.