MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
Rogers Arlon 25662T010 0.010" (0.254 mm) Cured Silicone Rubber with Laminated ETFE Film Substrate
Categories: Polymer; Thermoset; Silicone; Silicone Rubber

Material Notes: Design/Construction:
Side 1: Cured Silicone Rubber
Substrate: Laminated ETFE Film

Chemical Compatibility: (ETFE offers good chemical resistance to the following classes of chemicals) Alkalis, Organic and Inorganic acids, Amines, Epoxies, Aromatic compounds, Chlorine compounds, Ethers, Ketones, Esters, Alcohols and Hydrocarbons

Product Use: Chemically resistant, reusable vacuum bag material

Appearance: Translucent silicone rubber chemically bonded to fluoropolymer film

This data represents typical values for the production material. The data should not be used to write, or in place of, material specifications.

Information provided by Arlon Silicone Technologies Division; now a part of Rogers Corporation.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.20 g/ccSilicone; Arlon SQA-TMS-024
 1.70 g/ccLaminated ETFE Film; ASTM D792
Thickness 2.00 milSubstrate; Arlon SQA-TMS-003
 8.00 milSide 1; Arlon SQA-TMS-003
 10.0 milOverall; Arlon SQA-TMS-003
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 55Silicone; ASTM D2240
 67Laminated ETFE Film; ASTM D2240
Tensile Strength 1300 psiSilicone; ASTM D412
 6000 psiLaminated ETFE Film; ASTM D638
Elongation at Break 300 %Laminated ETFE Film; ASTM D638
 700 %Silicone; ASTM D412
Elongation at Yield 6 %
@Temperature 20.0 °C
Elastic Deformation of ETFE Film; ASTM D638
Tear Strength 225 pliArlon SQA-TMS-029
 9.00 pli
@Temperature 150 °C
[ppiw], Break Strength; Arlon SQA-TMS-008
 13.0 pli
@Temperature 100 °C
[ppiw], Break Strength; Arlon SQA-TMS-008
 23.0 pli
@Temperature 20.0 °C
[ppiw], Break Strength; Arlon SQA-TMS-008
 
Electrical PropertiesOriginal ValueComments
Dielectric Strength 200 V/milASTM D149
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 310 °F
Minimum Service Temperature, Air -60.0 °F
 
Processing PropertiesOriginal ValueComments
Shelf Life 60.0 Month
@Temperature 21.1 - 26.7 °C
From date of manufacture
 
Descriptive Properties
ColorTranslucent
Total Product Weight (oz/yd2)9.6Arlon SQA-TMS-025

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Dow C6-350LH ELASTOMER KIT
Dow C6-180 ELASTOMER KIT
Dow 5-8601 FLUOROSILICONE LSR, KIT
Dow 3-6891 1-PART SILICONE RUBBER ABRADABLE SEALANT COMPOUND
Dow 3-6655 THERMALLY CONDUCTIVE ELASTOMER, KIT

PARL132 / 125318

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.