MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Metal adhesives

(Viewing data as-entered. Click here to return)
Tra-Con Tra-Bond 342-3.5 Room Temperature Cure Epoxy Adhesive
Categories: Polymer; Adhesive; Thermoset; Epoxy

Material Notes: TRA-BOND 342-3.5 room temperature curing epoxy adhesive is designed for applications which require outstanding thermal shock properties. This adhesive may be used to bond semi-porous materials such as ferrite, where a physical, rather than a chemical, bond is required. TRA-BOND 342-3.5 is recommended for fiber optic (glass and plastic) assembly and repair applications and other high performance electronic and aerospace applications that include structural laminating, lens and prism assembly, and small volume optical potting. Fully cured TRA-BOND 342-3.5 provides excellent resistance to salt solutions, mild acids and alkalis and many other chemicals including petroleum solvents, lubricating oils and alcohol.

Information provided by Tra-Con Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Viscosity 5000 cPMixed
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 86
Adhesive Bond Strength 3800 psiLap shear, alum to alum
 
Thermal PropertiesOriginal ValueComments
CTE, linear 35.0 µm/m-°CBelow Tg
 180 µm/m-°CAbove Tg
Glass Transition Temp, Tg 71.0 °CUltimate Tg
 
Processing PropertiesOriginal ValueComments
Cure Time 1.00 hour
@Temperature 120 °C
 2.00 hour
@Temperature 95.0 °C
 4.00 hour
@Temperature 75.0 °C
 48.0 hour
@Temperature 25.0 °C
Shelf Life 12.0 Month
@Temperature 25.0 °C
In Kits
 12.0 Month
@Temperature -40.0 °C
PMF
 
Descriptive Properties
Working Life hours 8At 25°C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Tra-Con Tra-Bond 342-14T Low Viscosity Room Temperature Cure Epoxy Adhesive
Tra-Con Tra-Bond 342-1 Room Temperature Cure Epoxy Adhesive

PTRAC116 / 71044

Metal adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.