MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Chemically Resistant adhesives

(Viewing data as-entered. Click here to return)
Rogers Arlon Thermabond® 99000W008 Silicone Rubber/Fiberglass Laminate
Categories: Polymer; Adhesive; Thermoset; Rubber or Thermoset Elastomer (TSE); Silicone; Silicone Rubber

Material Notes: Low outgassing, thermally conductive, electrically insulating, Thermabond®. Bonds with primer. Liner: 1 mil FEP; Product: uncured silicone rubber; Carrier: 3 mil PTFE coated fiberglass.

Information provided by Arlon Silicone Technologies; now a part of Rogers Corporation.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.70 g/ccsilicone property; Arlon SQA-TMS-024
Thickness 8.00 miloverall; Arlon SQA-TMS-003
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 85silicone property; ASTM D2240
Tensile Strength, Ultimate 300 psisilicone property; ASTM D412
Elongation at Break 28 %silicone property; ASTM D412
Modulus of Elasticity 4.75 ksisilicone property; Arlon SQA-TMS-008
Poissons Ratio 0.50silicone property
Shear Modulus 65.0 ksisilicone property; ASTM D1002
Shear Strength 185 psisilicone property; ASTM D1002
 
Electrical PropertiesOriginal ValueComments
Dielectric Constant 3.8
@Frequency 1e+6 Hz
silicone property; IPC TM 650-2.5.5.3
Dielectric Strength 950 V/milASTM D149
Dissipation Factor 0.0028
@Frequency 1e+6 Hz
silicone property; IPC TM 650-2.5.5.3
 
Thermal PropertiesOriginal ValueComments
CTE, linear 110 µm/m-°C
@Temperature 20.0 °C
silicone property; ASTM E 831
Specific Heat Capacity 0.700 J/g-°Csilicone property; ASTM E 1461-1
Thermal Conductivity 1.50 W/m-Ksilicone property; ASTM E 1530
Maximum Service Temperature, Air 400 °F
Minimum Service Temperature, Air -100 °F
Glass Transition Temp, Tg -116 °Csilicone property; ASTM E 1356
 
Processing PropertiesOriginal ValueComments
Cure Time 15.0 min
@Pressure 0.345 MPa,
Temperature 121 °C
Shelf Life 6.00 Month
@Temperature 7.22 °C
 
Descriptive Properties
ColorWhite

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Resinlab® EP1282 Clear Unfilled Electronic Grade Epoxy Encapsulant
Rogers Arlon Thermabond® 99000W015 Silicone Rubber/Fiberglass Laminate
Overview of materials for Silicone Rubber
Overview of materials for Nylon 12
Overview of materials for Polyvinylidinefluoride (PVDF), Molded/Extruded

PARL044 / 79696

Chemically Resistant adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.