MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
ATI Allegheny Ludlum 06 Tool Steel, UNS T31506
Categories: Metal; Ferrous Metal; Tool Steel; Cold Work Steel; Oil-Hardening Steel

Material Notes: An oil hardening grade with a fine dispersion of graphitic carbon for improved machinability and resistance to galling. Typical applications include gages, punches, forming dies, jigs, and machine parts such as spindles, cams, arbor wear plates, bushings and guides.

Information provided by Allegheny Ludlum

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 7.67 g/ccBased on UNS number
 
Component Elements PropertiesOriginal ValueComments
Carbon, C 1.45 %
Iron, Fe 96 %as balance
Manganese, Mn 1.0 %
Silicon, Si 1.25 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Carpenter O6 Graphitic Tool Steel (AISI O6)
Crucible Steel HALGRAPH® Tool Steel, AISI O6
AISI Type O6 Tool Steel
Carpenter Stentor® Alloy Tool Steel (Oil-Hard) (AISI 02)
Latrobe Graph-Mo® Cold Work Tool Steel (ASTM O6)

NLT06 / 18043

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.