MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
Teknor Apex Sarlink® TPV 24445N Thermoplastic Vulcanizate
Categories: Polymer; Thermoplastic; Elastomer, TPE; Thermoplastic Vulcanizate Elastomer (TPV)

Material Notes: Notes: Sarlink 24445N is a high performance thermoplastic vulcanizate used in variety of consumer and industrial applications. This product is a medium hardness, low density, UV stabilized grade suitable for injection molding.

Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North America

Features: Light Stabilized; Low Density; Low Flow; Low Specific Gravity; Lubricated; Medium Hardness; Slip; Sunlight Resistant; UV Absorbing

Uses: Consumer Applications; Gaskets; Glazing: Grommets; Plugs; Shock Absorbing Pads; Tubing

RoHS Compliance: RoHS Compliant

Form: Pellets

Processing Method: Injection Molding

Information provided by Teknor Apex

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.930 g/ccASTM D792
Melt Flow 1.0 g/10 min
@Load 2.16 kg,
Temperature 230 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 45ASTM D2240
Tensile Strength at Break 430 psiASTM D412
Elongation at Break 300 %ASTM D412
 
Processing PropertiesOriginal ValueComments
Rear Barrel Temperature 260 - 300 °F
Middle Barrel Temperature 280 - 320 °F
Front Barrel Temperature 300 - 340 °F
Nozzle Temperature 340 - 380 °F
Melt Temperature 340 - 380 °F
Mold Temperature 70.0 - 100 °F
Back Pressure 25.0 - 200 psi
Cushion 0.150 - 1.00 in
Screw Speed 50 - 100 rpm
 
Descriptive Properties
AppearanceOpaque

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PTEKNQ1187 / 237678

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.