MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Teknor Apex Medalist® MD-17135 XRD1 Thermoplastic Elastomer
Categories: Polymer; Thermoplastic; Elastomer, TPE

Material Notes: Notes: Medalist MD-17135 XRD1 is a high performance thermoplastic elastomer designed for medical and healthcare applications requiring high elasticity and excellent moldability. Medalist MD-17135 XRD1 is a low hardness, low density grade, available in NAT and colors, which can be sterilized and exhibits excellent adhesion to polypropylene. This grade is suitable for injection molding processing.

Availability: Africa & Middle East; Europe; Asia Pacific; Latin America; North America

Features: Autoclave Sterilizable; Chemical Resistant; Ethylene Oxide Sterilizable; Good Adhesion; Good Moldability; Good Sterilizability; Good Toughness; Halogen Free; Low Density; Low Hardness; Low Specific Gravity; Lubricated; Radiation Sterilizable; Resilient; Slip; Without Fillers

Uses: Bushings; Closures; Disposable Hospital Goods; Flexible Grips; Grommets; Knobs; Medical/Healthcare Applications; Pharmaceuticals; Plugs; Rubber Replacement

Agency Ratings: ISO 10993 Part 5; ISO 13485

RoHS Compliance: RoHS Compliant

Form: Pellets

Processing Method: Injection Molding

Preliminary data. Information provided by Teknor Apex

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.885 g/ccASTM D792
Melt Flow 7.0 g/10 min
@Load 5.00 kg,
Temperature 200 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 40
@Time 5.00 sec
ASTM D2240
 42
@Time 1.00 sec
ASTM D2240
Tensile Strength at Break 590 psiDie C, 20 in/min; ASTM D412
Tensile Stress at Strain 165 psi
@Strain 50 %
Die C, 20 in/min; ASTM D412
 200 psi
@Strain 100 %
Die C, 20 in/min; ASTM D412
 310 psi
@Strain 300 %
Die C, 20 in/min; ASTM D412
Elongation at Break 600 %Die C, 20 in/min; ASTM D412
Tear Strength 124 pliDie C, 20 in/min; ASTM D624
Compression Set 16 %
@Temperature 22.8 °C,
Time 79200 sec
Type 1; ASTM D395
 28 %
@Temperature 70.0 °C,
Time 79200 sec
Type 1; ASTM D395
 
Processing PropertiesOriginal ValueComments
Rear Barrel Temperature 320 - 350 °F
Middle Barrel Temperature 360 - 400 °F
Front Barrel Temperature 380 - 420 °F
Nozzle Temperature 360 - 440 °F
Melt Temperature 360 - 440 °F
Mold Temperature 80.0 - 120 °F
Back Pressure 50.0 - 150 psi
Cushion 0.150 - 0.500 in
Screw Speed 50 - 100 rpm
 
Descriptive Properties
AppearanceColors Available
 Natural Color
 Opaque

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
ASTM A709 Steel, grade 50 and 50W, ≤ 100 mm
ASTM A709 Steel, grade 50
AISI 1005 Steel

PTEKNQ0710 / 237201

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.