MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

CRP  Windform

(Viewing data as-entered. Click here to return)
Clariant Acrylonitrile Butadiene Styrene, White 3D Printer Filament
Categories: Polymer; 3D Printing/Additive Manufacturing Polymer; Thermoplastic; ABS Polymer

Material Notes: Clariant Acrylonitrile Butadiene Styrene (ABS) 3D printer filament is made of a high quality and good flowing ABS combined with Clariant additives and pigments to ensure high material performance, end use stability and outstanding color.

General properties:

  • Strong impact resistance
  • High toughness and durability
  • Strong heat resistance
  • High tensile strength
Optimized benefits:
  • Improved lubricity for better printability
  • Reduced thermo-oxidative degradation
  • Minimized undesired yellowing due to ultraviolet radiation
Applications:
  • Mechanical and technical application parts
  • Models
  • Prototypes

Information provided by Clariant.

Vendors:
Proto3000 provides design tools, 3D printers, additive manufacturing processes, metrology technologies, high-performance materials, and part-finishing automation. Our ISO 9001:2015 additive manufacturing production facility offers 3D printing services, rapid prototyping services, and end-part production with HP MultiJet Fusion (MJF), FDM, SLA, SLS, Polyjet, DLP, metal binder jetting, BMD, and DMLS.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Density 1.077 g/ccISO 1183
Melt Flow 3.7 g/10 min
@Load 2.16 kg,
Temperature 230 °C
ISO 1133
 34 g/10 min
@Load 10.0 kg,
Temperature 220 °C
ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 43.0 MPaInjection molded, 50 mm/min; ISO 527
Tensile Strength, Yield 43.0 MPaInjection molded, 50 mm/min; ISO 527
Elongation at Break 14 %Injection molded, 50 mm/min; ISO 527
Modulus of Elasticity 2.455 GPaInjection molded, 1 mm/min; ISO 527
Flexural Strength 66.0 MPaInjection molded; ISO 178
Flexural Modulus 2350 MPaInjection molded; ISO 178
Izod Impact, Notched (ISO) 84.0 kJ/m²Injection molded; ISO 180
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 83.0 °CInjection molded; ISO 75
 98.0 °C3D printed XY / flat at 230°C; ISO 75
Deflection Temperature at 1.8 MPa (264 psi) 73.0 - 78.0 °CInjection molded; ISO 75
 96.0 °C3D printed XY / flat at 230°C; ISO 75
 
Processing PropertiesOriginal ValueComments
Processing Temperature 230 - 240 °CPrint Temperature
 
Descriptive Properties
Bed AdhesionPET or Polyimide tape surface coated with a mixture of ABS dissolved in Acetone or directly onto a PEI surface
Bed Temperatureideally heated up to 110°C and ideally in an enclosed chamber to minimize warping
Fan Settingslow to medium
Print Speed30-50 mm/s
Volume5.28 cm3ISO 1183

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Clariant Natural Color Acrylonitrile Butadiene Styrene 3D Printer Filament
Clariant Acrylonitrile Butadiene Styrene Black 3D Printer Filament
Clariant Polycarbonate + ABS White 3D Printer Filament
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Molded
Clariant Polylactic Acid White 3D Printer Filament

PCLAR00009 / 232086

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.