MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Teknor Apex Monprene® SP-19985 XRD2 Thermoplastic Elastomer
Categories: Polymer; Thermoplastic; Elastomer, TPE

Material Notes: Notes: Monprene SP-19985 XRD2 is a high performance thermoplastic elastomer designed for a variety of consumer sporting good application including playground flooring requiring a soft, rubber-like feel. Monprene SP-19985 XRD2, available in NAT and colors, is a higher hardness, medium density, UV stabilized grade that exhibit excellent abrasion resistance and is suitable for injection molding.

Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North America

Features: Abrasion Resistant; Brominated; Filled; Flame Retardant; Good Colorability; High Flow; Medium Density; High Hardness; Light Stabilized; Lubricated; High Flow; Slip; Sunlight Resistant; UV Resistant

Uses: Flooring; Rubber Replacement

RoHS Compliance: RoHS Compliant

Form: Pellets

Processing Method: Injection Molding

Preliminary data. Information provided by Teknor Apex

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.02 g/ccASTM D792
Melt Flow 24 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 85
@Time 5.00 sec
Injection Molded; ASTM D2240
 87
@Time 1.00 sec
Injection Molded; ASTM D2240
Tensile Strength at Break 1320 psiDie C, 20 in/min, Across Flow; ASTM D412
 1440 psiDie C, 20 in/min, Flow; ASTM D412
Tensile Stress at Strain 706 psi
@Strain 100 %
Die C, 20 in/min, Across Flow; ASTM D412
 837 psi
@Strain 100 %
Die C, 20 in/min, Flow; ASTM D412
 917 psi
@Strain 300 %
Die C, 20 in/min, Across Flow; ASTM D412
 1080 psi
@Strain 300 %
Die C, 20 in/min, Flow; ASTM D412
Elongation at Break 500 %Die C, 20 in/min, Flow; ASTM D412
 600 %Die C, 20 in/min, Across Flow; ASTM D412
Tear Strength 213 pliDie C, 20 in/min, Across Flow; ASTM D624
 256 pliDie C, 20 in/min, Flow; ASTM D624
Compression Set 40 %
@Temperature 22.8 °C,
Time 79200 sec
Type 1; ASTM D395B
 71 %
@Temperature 70.0 °C,
Time 79200 sec
Type 1; ASTM D395B
 
Thermal PropertiesOriginal ValueComments
Oxygen Index 20 %ASTM D2863
 
Processing PropertiesOriginal ValueComments
Rear Barrel Temperature 380 - 420 °F
Middle Barrel Temperature 380 - 420 °F
Front Barrel Temperature 380 - 420 °F
Nozzle Temperature 380 - 420 °F
Melt Temperature 380 - 420 °F
Mold Temperature 60.0 - 90.0 °F
Injection Pressure 200 - 1000 psi
Back Pressure 25.0 - 50.0 psi
Cushion 0.150 - 1.00 in
Screw Speed 50 - 100 rpm
 
Descriptive Properties
AppearanceBlue
 Natural Color

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PTEKNQ0964 / 237455

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.