MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Metal adhesives

(Viewing data as-entered. Click here to return)
Resinlab® AR 4305 HP Metal Bonding Methacrylate Adhesive
Categories: Polymer; Adhesive; Thermoset; Methacrylate; Methacrylate Adhesive

Material Notes: Resinlab™ AR 4305 HP is a 1:1 mix methacrylate-based structural adhesive designed for general purpose bonding of a wide variety of materials in industrial applications. AR 4305 HP forms tough, durable bonds to most plastics, composites, metals, ceramics. It contains special adhesion promoters to enhance performance on hard to bond materials such as nylon, chrome and rubber. Surface cleaning or preparation, or the use of primers, or chemical wipes is not required in almost all cases. It has excellent adhesion to as received metals such as aluminum, stainless, galvanized and plated steels. The cure time was designed for high speed manufacturing processes where fast fixturing is required. AR 4305 HP is easily dispensed from packaged cartridges or with commercial dispensing equipment as a non-sag, creamy gel, with no stringing. The product was designed to be used with static mixer tubes and has a balanced viscosity between parts. There are no abrasive fillers or extenders to reduce performance or cause wear in dispensing equipment.

Information Provided by Resinlab L.L.C., an Ellsworth Adhesives Company.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Viscosity 250000 cPPart A, Spindle TD, 2.5 rpm; Uncured
 280000 cPSpindle TD, 2.5 rpm; Curing
 300000 cPPart B, Spindle TD, 2.5 rpm; Uncured
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 65Cured
Elongation at Yield 15 %Cured
Adhesive Bond Strength 3500 psialum/aluminum
 4000 psisteel/steel
Impact >= 13[J/in^2]; FRP/FRP; auto side impact
Peel Strength >= 30.0 plisteel/steel
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 250 °FCured
Minimum Service Temperature, Air -40.0 °F
Flash Point 51.0 °FLCC; Uncured
 
Descriptive Properties
ColorAmberPart B; Uncured
 Off WhitePart A; Uncured
Fixture Time (minutes)9-10Curing
Mix Ratio1:1Weight and Volume; Uncured
Working Time (minutes)5-6Curing

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PRESL002 / 101416

Metal adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.