MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
SABIC SABIC® LLDPE 218BJ PE (Asia)
Categories: Polymer; Thermoplastic; Polyethylene (PE); Linear Low Density (LLDPE)

Material Notes: SABIC® LLDPE 218BJ is a butene linear low density polyethylene resin with an additive package typically designed for a broader range of food applications (TNPP free). The good thermal stability allows to use the resin in critical extrusion processing conditions. Films produced from SABIC® LLDPE 218BJ have better draw-down ability compared to lower MFR LLDPE resins. This product is not intended for and must not be used in any pharmaceutical/medical applications.

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.918 g/ccASTM D1505
Melt Flow 2.0 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Film Tensile Strength at Yield, MD 12.0 MPaProperties have been measured by producing 30 µm film with 2.5 BUR using 100% 218BJ.; ASTM D882
Film Tensile Strength at Yield, TD 10.0 MPaProperties have been measured by producing 30 µm film with 2.5 BUR using 100% 218BJ.; ASTM D882
Film Elongation at Break, MD 550 %Properties have been measured by producing 30 µm film with 2.5 BUR using 100% 218BJ.; ASTM D882
Film Elongation at Break, TD 670 %Properties have been measured by producing 30 µm film with 2.5 BUR using 100% 218BJ.; ASTM D882
Puncture Energy 60.0 JJ/m; Properties have been measured by producing 30 µm film with 2.5 BUR using 100% 218BJ.; SABIC method
Elmendorf Tear Strength MD 135 gProperties have been measured by producing 30 µm film with 2.5 BUR using 100% 218BJ.; ASTM D1922
Elmendorf Tear Strength TD 400 gProperties have been measured by producing 30 µm film with 2.5 BUR using 100% 218BJ.; ASTM D1922
Dart Drop 110 g/micronProperties have been measured by producing 30 µm film with 2.5 BUR using 100% 218BJ.; ASTM D1709
Film Tensile Strength at Break, MD 31.0 MPaProperties have been measured by producing 30 µm film with 2.5 BUR using 100% 218BJ.; ASTM D882
Film Tensile Strength at Break, TD 22.0 MPaProperties have been measured by producing 30 µm film with 2.5 BUR using 100% 218BJ.; ASTM D882
1% Secant Modulus, MD 200 MPaProperties have been measured by producing 30 µm film with 2.5 BUR using 100% 218BJ.; ASTM D882
1% Secant Modulus, TD 240 MPaProperties have been measured by producing 30 µm film with 2.5 BUR using 100% 218BJ.; ASTM D882
 
Thermal PropertiesOriginal ValueComments
Vicat Softening Point 98.0 °CASTM D1525
 
Optical PropertiesOriginal ValueComments
Haze 7.0 %
@Thickness 0.0300 mm
2.5 BUR using 100% 218BJ.; ASTM D1003
Gloss 80 %60°; Properties have been measured by producing 30 µm film with 2.5 BUR using 100% 218BJ.; ASTM D2457

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSABI11045 / 244512

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.