MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Envalior Durethan® BKV 60 EF DUS097 000000 Nylon 6 (PA6), 60% Glass Fiber Reinforced, Dry
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, 60% Glass Fiber Filled

Material Notes: PA 6, 60% glass fibers, injection molding, improved flowability, heat-aging stabilized

Former Lanxess product line is now with Envalior.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Moisture Absorption at Equilibrium 1.18 %50% RH; ISO 62
Water Absorption at Saturation 3.75 %IOS 62
Linear Mold Shrinkage, Flow 0.0030 cm/cm60x60x2; 280 °C / MT 80°C; 600 bar; ISO 294-4
Linear Mold Shrinkage, Transverse 0.0060 cm/cm60x60x2; 280 °C / MT 80°C; 600 bar; ISO 294-4
 
Mechanical PropertiesOriginal ValueComments
Puncture Resistance 1346 N
@Temperature -30.0 °C
ISO 6603-2
 1476 N
@Temperature 23.0 °C
ISO 6603-2
Tensile Strength at Break 230 MPa5 mm/min; ISO 527-1,-2
Elongation at Break 2.5 %5 mm/min; ISO 527-1,-2
Tensile Modulus 19500 MPa1 mm/min; ISO 527-1,-2
Flexural Strength 390 MPa2 mm/min; ISO 178-A
Flexural Modulus 20000 MPa2 mm/min; ISO 178-A
Flexural Strain at Break 3.0 %2 mm/min; ISO 178-A
Izod Impact, Notched (ISO) 18.0 kJ/m²
@Temperature 23.0 °C
ISO 180-1A
 18.0 kJ/m²
@Temperature -30.0 °C
ISO 180-1A
Izod Impact, Unnotched (ISO) 90.0 kJ/m²
@Temperature 23.0 °C
ISO 180-1U
 95.0 kJ/m²
@Temperature -30.0 °C
ISO 180-1U
Charpy Impact Unnotched 95.0 kJ/m²
@Temperature 23.0 °C
ISO 179-1eU
Charpy Impact, Notched 17.0 kJ/m²
@Temperature 23.0 °C
ISO 179 1eA
 17.0 kJ/m²
@Temperature -30.0 °C
ISO 179 1eA
Puncture Energy 3.80 J
@Temperature -30.0 °C
ISO 6603-2
 4.30 J
@Temperature 23.0 °C
ISO 6603-2
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 10.0 µm/m-°C
@Temperature 23.0 - 55.0 °C
ISO 11359-1,-2
CTE, linear, Transverse to Flow 80.0 µm/m-°C
@Temperature 23.0 - 55.0 °C
ISO 11359-1,-2
Melting Point 221 °C10°C/min; ISO 11357-1,-3
Deflection Temperature at 0.46 MPa (66 psi) 220 °CISO 75-1,-2
Deflection Temperature at 1.8 MPa (264 psi) 213 °CISO 75-1,-2
Deflection Temperature at 8.0 MPa 186 °CISO 75-1,-2
Shrinkage, MD 0.030 %
@Treatment Temp. 120 °C,
Time 14400 sec
Post-Shrinkage Flow Direction; 60x60x2; ISO 294-4
Shrinkage, TD 0.020 %
@Treatment Temp. 120 °C,
Time 14400 sec
60x60x2; ISO 294-4
 
Processing PropertiesOriginal ValueComments
Melt Temperature 280 °Cinjection molding
 270 - 290 °C
Mold Temperature 80.0 °Cinjection molding
 80.0 - 120 °C
Drying Temperature 80.0 °C
Dry Time 2.00 - 6.00 hour
Moisture Content 0.060 - 0.20 %Karl Fischer

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Covestro Bayblend® T65 XF Polycarbonate + ABS
Kolon Kocetal® K300 General Purpose Grade Acetal Copolymer
Envalior Akulon® Ultraflow™ K-FHG12 Nylon 6-60% Glass Reinforced (European and Asian Grade) (Dry)
BASF Ultramid® KR 4355 G10 BK 23215 50% Glass Filled PA6/6T (Conditioned)

PLANW9432 / 208263

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.