MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Eastman Piccotac™ 1100 Hydrocarbon Resin
Categories: Polymer

Material Notes: Product Description: Piccotac™ 1100 hydrocarbon resin is a 100°C softening point, thermoplastic, low molecular weight, aliphatic C5 resin. Derived largely from mixed monomers of petroleum origin, it is characterized by its light color, excellent balance of tack and of adhesive and cohesive properties, heat resistance, and wide compatibility and solubility. Piccotac™ 1100 hydrocarbon resin is stabilized by addition of 0.10% antioxidant. It is designed primarily for use in pressure sensitive adhesives and hot melt adhesives and coatings.

Application/Uses:

  • Automotive refinish
  • Building and Construction
  • Hot Melt Adhesives
  • Nonwovens
  • Packaging
  • Pressure sensitive adhesives
  • Solventborne Adhesives
  • Tapes and Labels
  • Wax Modification
Key Attributes:
  • Aliphatic C5 resin
  • Excellent adhesion to natural rubber based adhesives
  • Excellent color and color stability
  • Excellent peel and tack properties
  • Limited compatibility with styrene-isoprenestyrene (SIS) block copolymersInformation provided by Eastman
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Viscosity 1000 cP
@Temperature 170 °C
Melt
 10000 cP
@Temperature 135 °C
Melt
 100000 cP
@Temperature 120 °C
Melt
Molecular Weight 950 g/molMn
 2900 g/molMw. Mw/Mn ratio = 3
 8250 g/molMz
 
Thermal PropertiesOriginal ValueComments
Glass Transition Temp, Tg 46.0 °C
Ring & Ball Softening Point 100 °CASTM E28
 
Optical PropertiesOriginal ValueComments
Gardner Color Number 3.0
 
Descriptive Properties
Cloud Point62°CDACP
 96°CMMAP

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PEATM5512 / 222706

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.