MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
TSE Industries EcoWIND® M110 General Purpose Filament Winding Polyurethane Resin
Categories: Polymer; Thermoset; Polyurethane, TS; Thermoset Polyurethane, Liquid

Material Notes: TSE-EcoWIND® resins are “Environmentally-Preferred Products” or EPP’s. They are a pair of polyurethane resins free of Styrene, and are “ultra-low” emitting during application. TSE-EcoWIND® resins are formulated for filament winding applications serving the composite pressure vessel, tank, and piping markets. These PU resins have tested positively in both hot and cold pressure vessel applications and can be applied to reinforce thermoplastic substrates (i.e. polyethylene, ABS, etc.) or applied directly to a release coated mandrel surface.

All information provided by TSE Industries

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Viscosity 100 - 400 cP
@Temperature 45.0 °C
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength 66.0 MPaPlain Cast Resin; ASTM D638
Elongation at Break 3.5 - 4.5 %Plain Cast Resin; ASTM D638
Modulus of Elasticity 3.20 GPaPlain Cast Resin; ASTM D638
Flexural Yield Strength 97.5 MPaPlain Cast Resin; ASTM D790
Flexural Modulus 2.70 GPaPlain Cast Resin; ASTM D790
Izod Impact, Notched 4.30 J/cmPlain Cast Resin; ASTM D256
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 1.8 MPa (264 psi) 54.0 °CPlain Cast Resin; ASTM D648
Glass Transition Temp, Tg 83.0 °CPlain Cast Resin; ASTM D3418
 
Processing PropertiesOriginal ValueComments
Pot Life 15.0 - 20.0 min
@Temperature 23.0 °C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Coastal Enterprises Plus™ PBHT-15 High Density Urethane Foam
Alliance Polymers Zythane™ 3045D Thermoplastic Polyurethane Elastomer
Covestro Baydur® 110 FR Polyurethane
Overview of materials for Thermoset Polyurethane, Liquid
TSE Industries EcoWIND® 100 Polyurethane Resin Filament Winding

PMILL000c / 159590

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.