MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
3M Novec™ 7100 Engineered Fluid
Categories: Fluid

Material Notes: 3M™ Novec™ 7100 Engineered Fluid, methoxy-nonafluorobutane (C4F9OCH3), is a clear, color less and low-odor fluid intended to replace ozone-depleting substances (ODSs) and compounds with high global warming potential (GWP) in many applications. Its physical properties are compared with several other ODS replacement fluid candidates in Table 1. This proprietary fluid has zero ozone depletion potential and other favorable environmental properties (see Table 2). It has one of the best toxicological profiles of CFC replacement materials, with a time-weighted average exposure guideline of 750 ppm (eight hour average). The high boiling point and low surface tension of Novec 7100 fluid make it ideal for use in vapor degreasing applications as a neat (pure), azeotropic component or co-solvent parts cleaner. In addition, its chemical and thermal stability, non-flammability and low toxicity make it useful for many other industrial and specialty solvent applications.

Typical Applications:

  • Cleaning and rinsing agent, Heavy-duty cleaning (co-solvent)– heavy oils, greases, fluxes Medium-duty cleaning (azeotrope)– oils, greases, waxes, Light-duty cleaning (neat)– particulates, fluorolubes, light oils, fluoropolymers
  • Lubricant carrier, Fluorocarbons, Hydrocarbons, Silicones
  • Spot-free water drying agent (with surfactants added)
  • Specialty solvents, dispersion media, reaction media
  • Spray contact cleaner
  • CFC, HCFC, HFC and PFC replacement
  • Dielectric test media
  • Heat transfer See “3M™ Novec™ 7100 Engineered Fluid for Heat Transfer” Application Information

Information provided by 3M

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.538 g/cc
Molecular Weight 250 g/mol
Surface Tension 13.6 dynes/cm
 
Thermal PropertiesOriginal ValueComments
Boiling Point 61.0 °C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
3M Novec™ 7000 Engineered Fluid
3M Novec™ 649 Engineered Fluid
3M Novec™ 774 Engineered Fluid
3M Novec™ 7100DL Engineered Fluid
3M Novec™ 71DA Engineered Fluid

PMM33100 / 167847

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.