MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
BYK ADD-VANCE® CL 510 Clarification Masterbatch with Random Copolymer PP carrier  (discontinued **)
Categories: Other Engineering Material; Additive/Filler for Polymer; Polymer; Thermoplastic; Polypropylene (PP)

Material Notes: Fields of application: Extrusion blow molding, film or fiber extrusion, (thinwall) injection molding, sheet extrusion and thermoforming of PP resins (both homopoloymer and random copoloymer).
Examples: Beverage and food packaging, housewares, appliance parts, medical packaging, media packaging, office supplies, protective packaging, BOPP film.

ADD-VANCE® CL 510 contains a ‘third generation’ clarifying agent. This clarifying agent increases the rate of crystal initiation by many orders of magnitude, resulting in many more crystals of smaller size. The result is crystals smaller than the wavelength of visible light that allow light to pass through, thus offering enhanced clarity. Due to the strong nucleating effect of the active ingredient, increased barrel temperatures may be necessary to ensure complete mold fill. Polished mold surfaces are necessary to achieve clarity. As the active ingredient is not compatible with many nucleating agents, it is recommended to use ADD-VANCE® CL 510 only in combination with unnucleated PP resins.

Advantages: Good clarity, gloss and surface smoothness in PP; Higher throughputs; Improved physical properties: e.g. higher stiffness and heat distortion temperature; Improved chemical and heat resistance, also acts as a moisture barrier; No taste, no odor; No plate-out on cooling surfaces; Low material density; Microwavability; Superior hot fill properties; Significant cost savings compared to other material options; Non-sticking pellets, dust free dosing; and Safe and easy handling.

Regulations: ADD-VANCE® CL 510 is suitable for food contact applications, e.g. cleared for food contact applications by the FDA, HPB and BGA.

Former ADDCOMP product line, acquired by BYK.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Processing PropertiesOriginal ValueComments
Processing Temperature <= 270 °C
 
Descriptive Properties
AppearanceWhite/off-white granules
Dosing Level2-2.5%

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
A. Schulman POLYBATCH™ White P8555 SC Concentrate Based In Random Copolymer Polypropylene
A. Schulman POLYBATCH™ ABPP-05 Antiblock Concentrate
A. Schulman POLYBATCH™ White P8555 T2 Concentrate Based In Homopolymer Polypropylene
Borealis Xmod™ HF006SA High Stiffness Polypropylene for Injection Molding Applications
Formosa Plastics Formolene® 5140L Homopolymer Polypropylene

PPADDC48 / 133261

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.