Alloy 165 plate from Materion provides strength close to that of Alloy 25, with slightly lower beryllium content. This alloy features high fatigue strength and resistance to wear, corrosion, galling and stress relaxation. Typical applications include wear plates and resistance welding components.Information provided by Materion. |