Hostacom ERC 161N C1 Natural is a mineral filled, polypropylene copolymer for injection molding. It combines excellent stiffness/impact balance, low odor and excellent flowability properties with good dimensional stability. The grade has been specifically designed for molding of automotive interior trim parts. The grade is available in color-matched, pellet form. Applications: Interior TrimsInformation provided by LyondellBasell. |