MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Copper, UNS C15710, 0.8 mm wire, 65% Cold Worked
Categories: Metal; Nonferrous Metal; Copper Alloy

Material Notes: Excellent cold workability. Fabricated by extrusion, drawing, rolling, impacting, heading, swaging, bending, machining, blanking, roll threading.

Applications: electrical connectors, light-duty current-carrying springs, inorganic insulated wire, thermocouple wire, lead wire, resistance welding electrodes for aluminum, heat sinks.

Test specimen: wire - 0.8 mm diameter; 65% cold worked.

Inactive per the Copper Development Association.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 8.82 g/cc
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Ultimate 455 MPa
Tensile Strength, Yield 420 MPa
@Strain 0.2 %
Modulus of Elasticity 105 GPa
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.00000192 ohm-cm
@Temperature 20.0 °C
 
Thermal PropertiesOriginal ValueComments
CTE, linear 19.5 µm/m-°C
@Temperature 20.0 - 300 °C
Specific Heat Capacity 0.380 J/g-°C
Thermal Conductivity 360 W/m-K
Melting Point <= 1080 °C
Liquidus 1080 °C
 
Processing PropertiesOriginal ValueComments
Annealing Temperature 650 - 875 °C
 
Component Elements PropertiesOriginal ValueComments
Al2O3 0.15 - 0.25 %
Copper, Cu 99.69 - 99.85 %Specified
Iron, Fe <= 0.010 %
Lead, Pb <= 0.010 %
Oxygen, O <= 0.040 %Excluding Al2O3

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
United Cast Bar Unibar 250 Continuously Cast Iron
United Cast Bar Unibar 200 Continuously Cast Iron
Harris Acoustic Sensors EC-65 Lead Zirconium Titanate Piezoelectric
H.C. Starck Amperit® 568.062 Tungsten Carbide-Nickel 92-8 - Nickel SF RC 60 65-35
H.C. Starck Amperit® 568.005 Tungsten Carbide-Nickel 92-8 - Nickel SF RC 60 65-35

MC15710c4 / 10678

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.