MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
Materion AyontEX™ 13 Aluminum Alloy Matrix
Categories: Metal; Metal Matrix Composite; Nonferrous Metal; Aluminum Alloy

Material Notes: AyontEX™ alloys are a series of hypereutectic aluminum-silicon alloys containing micron-sized silicon particles in an aluminum alloy matrix. This ultrafine reinforcement provides several key benefits: high specific stiffness and strength, reduced coefficient of thermal expansion (CTE), excellent fatigue performance, improved damping, low friction and outstanding wear resistance. The applications for AyontEX alloys are varied and include mirrors, support structures, optical housings, electronic housings, waveguide structures, adapters and interface components.

Information provided by Materion.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 2.54 g/cc
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Ultimate 50.0 ksi
Tensile Strength, Yield 49.0 ksi
@Strain 0.200 %
Modulus of Elasticity 103 GPa
Poissons Ratio 0.300
Shear Modulus 40.0 GPaCalculated
 
Thermal PropertiesOriginal ValueComments
CTE, linear 7.20 µin/in-°F
@Temperature 20.0 - 50.0 °C
Specific Heat Capacity 0.850 J/g-°C
Thermal Conductivity 134 W/m-K
 
Descriptive Properties
Specific Stiffness41 GPa/g/cm3
Specific Strength136 MPa/g/cm3

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

NBB92188 / 323546

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.