MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Konson MB-80 Masterbatch
Categories: Other Engineering Material; Additive/Filler for Polymer

Material Notes: Composition: 80%2-mercaptobenzimidazole 20% EPDM/EVA binder and dispersing agents

Use Characteristics: Konson® MB-80 is a non-staining antioxidant for light-coloured and white rubber compounds. It is used as a synergist for other antioxidants. The effect of the combination of Konson® MB-80 with other antioxidants is greater than the sum of the effects of the individual components. The combination of Konson®MB-80 with antiozonant IPPD is suitable for extremely heat resistant vulcanizates. It also provides the vulcanizates with some protection against copper and manganese poisoning. The efficiency of Konson® MB-80, used on its own, depends to a large extent on the curing system. Konson® MB-80 gives better results in combination with dithiocarbamate and thiuram accelerators than in combination with other accelerators.

Processing Advantages: The thermoplastic, excellent compatible EPDM/EVA binder which is combined with active dispersing promoters allows much more easily and quickly incorporation and excellent dispersion in the rubber mixing. In this way, optimal activity of the effective MB is assured.

Dosage levels: As antioxidant: 0.6 - 1.5 phr As antioxidant, specially for steam-resistant grades: 2.0 - 3.0 phr for transparent grades: 0.4 phr.

Applications: Rubber articles which must withstand oxygen, heat and steam; heat-resistant rubber articles which are produced by thiuram vulcanization; white, coloured and transparent articles of all kinds; fabric proofings.

Information provided by Konson®

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.27 g/cc
Ash <= 0.50 %
Evaporation Loss <= 0.50 %
 
Thermal PropertiesOriginal ValueComments
Melting Point 290 °C
 
Descriptive Properties
AppearanceWhite-grey granules
Content= 98%MB

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PKONS014 / 256059

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.