MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Wacker Vinnapas® AF 75 Polymer Dispersion
Categories: Polymer; Thermoplastic; Ethylene Vinyl Acetate

Material Notes: Product description: VINNAPAS® AF 75 is an aqueous, plasticizer-free polymer dispersion produced from acrylic ester monomers.

Properties: Considering that VINNAPAS® AF 75 is a pressure sensitive adhesive with very high surface tack, it exhibits excellent cohesion and adhesion even at elevated temperatures.

Special features: Notable features of VINNAPAS® AF 75 are:

  • high surface tack
  • very good adhesion at low temperatures
Application: VINNAPAS® AF 75 can be used to manufacture pressure sensitive adhesives, adhesives for self adhesive insulation materials (e.g. bitumen sheets, automotive insulation felt), special adhesive tapes, plastic films and paper labels.

Information provided by Wacker Chemie AG.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Solids Content 59 - 61 %DIN EN ISO 3251
pH 4.8 - 6.0DIN/ISO 976
Viscosity 3500 - 6500 cPdynamic; DIN EN ISO 2555
 
Thermal PropertiesOriginal ValueComments
Glass Transition Temp, Tg -60.0 °C
 
Optical PropertiesOriginal ValueComments
Transmission, Visible 90 %"Clear" but manufacturer does not quantify.
 
Descriptive Properties
Appearanceclear, glossy

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Celanese Ateva® 1922A GROUND Ethylene Vinyl Acetate Copolymer

PWACK9621 / 205150

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.