MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
PTS PCA-1012 High Impact Polycarbonate/ABS Alloy
Categories: Polymer; Thermoplastic; ABS Polymer; Polycarbonate/ABS Alloy, Unreinforced; Polycarbonate (PC)

Material Notes: Information provided by Polymer Technology and Services, LLC (PTS).

Key Words: PC+ABS; Poly(Acrylonitrile Butadiene Styrene)
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.14 g/ccASTM D792
Water Absorption 0.10 %24 hours at 73°F; ASTM D570
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 55.2 MPa
@Thickness 3.17 mm
ASTM D638
Elongation at Break 125 %
@Thickness 3.17 mm
ASTM D638
Flexural Yield Strength 82.7 MPa
@Thickness 3.17 mm
ASTM D790
Flexural Modulus 2.21 GPa
@Thickness 3.17 mm
ASTM D790
Izod Impact, Notched 6.41 J/cm
@Thickness 3.17 mm
ASTM D256
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 1.8 MPa (264 psi) 102 °CASTM D648
 
Processing PropertiesOriginal ValueComments
Rear Barrel Temperature 430 - 445 °F
Middle Barrel Temperature 435 - 455 °F
Front Barrel Temperature 445 - 465 °F
Nozzle Temperature 450 - 470 °F
Melt Temperature 460 - 490 °F
Mold Temperature 155 - 190 °F
Drying Temperature 220 °F
Dry Time 2 - 4 hour
Injection Pressure 10000 - 20000 psi
Back Pressure 50.0 - 100 psi
Shot Size 50 - 80 %
Screw Speed 40 - 70 rpm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
PTS PCA-1011 High Impact Polycarbonate/ABS Alloy
Covestro Bayblend® SF 1443 Polycarbonate + ABS Blend Structural Foam
PTS PCA-1010HF High Flow Polycarbonate/ABS Alloy
Overview of materials for PC/ABS + Stainless Steel
Dow AIM® 4800 High Impact Styrenic Resin

PZ9PU42 / 21577

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.