MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
SABIC LNP™ LUBRICOMP™ Compound DFL36ELH Polycarbonate (PC)
Categories: Polymer; Thermoplastic; Polycarbonate (PC)

Material Notes: LNP LUBRICOMP DFL36ELH compound is based on Polycarbonate (PC) resin containing 30% glass fiber, 15% PTFE. Added features of this grade include: Wear Resistant, Low Extractable, Easy Molding, Healthcare.

Features: Low Extractable,Healthcare,Wear resistant,Food Contact Acceptable,Easy Molding,Structural

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.55 g/ccASTM D792
 1.55 g/ccISO 1183
Moisture Absorption 0.0200 %Injection Molding
Linear Mold Shrinkage, Flow 0.0010 - 0.0030 cm/cm24hrs; ASTM D955
 0.0021 cm/cm24hrs; ISO 294
Linear Mold Shrinkage, Transverse 0.0060 - 0.0080 cm/cm24hrs; ASTM D955
 0.0071 cm/cm24hrs; ISO 294
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 112 MPaASTM D638
 113 MPaISO 527
Tensile Strength, Yield 113 MPaASTM D638
 114 MPaISO 527
Elongation at Break 2.5 %ASTM D638
 2.6 %ISO 527
Elongation at Yield 2.4 %ASTM D638
 2.4 %ISO 527
Tensile Modulus 9280 MPa1 mm/min; ISO 527
 9650 MPa50 mm/min; ASTM D638
Flexural Strength 179 MPaASTM D790
 180 MPaISO 178
Flexural Modulus 8700 MPaISO 178
 8960 MPaASTM D790
Izod Impact Notched 176 JASTM D256
Izod Impact, Unnotched 854 J/mASTM D4812
Izod Impact, Notched (ISO) 17.0 kJ/m²80*10*4; ISO 180/1A
Izod Impact, Unnotched (ISO) 51.0 kJ/m²80*10*4; ISO 180/1U
Dart Drop, Total Energy 21.0 Jpeak; ASTM D3763
Impact Test 7.00 JMultiaxial Impact; ISO 6603
Coefficient of Friction, Dynamic 0.57ASTM D3702 Modified: Manual
Coefficient of Friction, Static 0.49ASTM D3702 Modified: Manual
K (wear) Factor 27.0 x 10-10 in³-min/ft-lb-hrWasher; ASTM D3702 Modified: Manual
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 30.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
ISO 11359-2
 30.6 µm/m-°C
@Temperature -40.0 - 40.0 °C
ASTM E831
CTE, linear, Transverse to Flow 46.8 µm/m-°C
@Temperature -40.0 - 40.0 °C
ASTM E831
 47.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
ISO 11359-2
Deflection Temperature at 0.46 MPa (66 psi) 149 °CFlatw 80*10*4 sp=64mm; ISO 75/Bf
 147 °C
@Thickness 3.20 mm
unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 144 °CFlatw 80*10*4 sp=64mm; ISO 75/Af
 142 °C
@Thickness 3.20 mm
unannealed; ASTM D648
 
Processing PropertiesOriginal ValueComments
Zone 2 310 - 320 °C
Zone 3 320 - 330 °C
Melt Temperature 305 - 325 °CInjection Molding
Mold Temperature 80.0 - 110 °C
Drying Temperature 120 °CInjection Molding
Dry Time 4.00 hourInjection Molding
Back Pressure 0.200 - 0.300 MPa
Screw Speed 30 - 60 rpm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSABH80715 / 288662

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.