MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
ATI Allegheny Ludlum Stainless Steel Chromium-Nickel-Manganese AL 201LN™, M-7 (UNS S20153)
Categories: Metal; Ferrous Metal; Stainless Steel; T S20000 Series Stainless Steel

Material Notes: AL 201LN™ is a special composition of Type 201 specifically for sub-zero temperature service as welded tanks and vessels. This alloy has replaced the familiar 300 series stainless such as type 301 or type 304 in many applications based upon technical equivalency and economic considerations. AL 201LN alloy is a natural choice for use at temperatures down to -320°F. The alloy is suited for many ambient temperature structural applications, such as railroad freight cars, truck trailers, coal handling and other bulk transport equipment where there is need for a good combination of corrosion resistance, strength, toughness and ease of fabrication.

Information provided by Allegheny Ludlum Corporation.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 7.857 g/cc
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Ultimate 673 MPa
@Temperature 70.0 °C
transverse
Tensile Strength, Yield 321 MPa
@Temperature 70.0 °C
transverse
Elongation at Break 59 %
@Temperature 70.0 °C
transverse
Izod Impact 184 Jtransverse
 
Component Elements PropertiesOriginal ValueComments
Carbon, C <= 0.030 %
Chromium, Cr 16 - 17.5 %
Copper, Cu <= 1.0 %
Iron, Fe 71 %as balance
Manganese, Mn 6.4 - 7.5 %
Nickel, Ni 4.0 - 5.0 %
Nitrogen, N 0.10 - 0.25 %
Phosphorus, P <= 0.045 %
Silicon, Si <= 0.75 %
Sulfur, S <= 0.015 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
ATI Allegheny Ludlum Stainless Steel Chromium-Nickel-Manganese AL 201LN™, M-6 (UNS S20153)
Outokumpu 4372 Cr-Ni Austenitic Stainless Steel
ATI Allegheny Ludlum Stainless Steel Chromium-Nickel-Manganese AL 201LN™, M-8 (UNS S20153)
ASTM A572 Steel, grade 65
ASTM A441 Steel, 19-38 mm thick

NL20L1 / 17825

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.