Product Description: A high crystallinity, high stiffness, high impact copolymer resin designed for injection molding applications requiring medium melt flow rate, good processing characteristics and improved cycle time. Availability: North America and Asia Pacific Features: - Balanced Stiffness/Toughness
- Fast Molding Cycle
- Medium Flow
- High Impact Resistance
- High Stiffness
- Nucleated
Uses: - Appliance
- Automotive Applications
- Child Safety Seats
- Consumer Applications
- Industrial Applications
- Rigid Packaging
Processing Method: Injection MoldingAutomotive Specifications: Hyundai MS213-26 Type 1 (Approval specific to USA sourced material) Information provided by ExxonMobil Chemical |