MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Borealis TR503T Polypropylene, 10% Mineral Fiber Reinforced
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene Copolymer

Material Notes: This grade is characterized by excellent impact strength even at low temperatures combined with high stiffness and good flow properties. is a 10% mineral filled polypropylene compound intended for injection molding is a polypropylene homopolymer intended for injection molding.

Special Features:

  • impact strength at low temperature
Applications: TR503T has been developed especially for the automotive industry.
  • Bumpers
Values determined on standard injection molded specimens conditioned at 23°C and 50% relative humidity after at least 96 hours storage time. To avoid residual humidity from transport or storage, the material should be pre-dried approximately 2h at 95° - 105°C.

Information provided by Borealis AG

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.965 g/ccISO 1183
Melt Flow 13.0 g/10 min
@Load 2.16 kg,
Temperature 230 °C
ISO 1133
Storage Temperature <= 50.0 °C
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 85.0ISO 2039-2
Tensile Strength, Yield 17.0 MPa50 mm/min; ISO 527-2
Flexural Strength 22.0 MPaISO 178
Flexural Modulus 1100 MPa2 mm/min; ISO 178
Izod Impact, Notched (ISO) 5.00 kJ/m²
@Temperature -30.0 °C
ISO 180/1A
 15.0 kJ/m²
@Temperature 0.000 °C
ISO 180/1A
 35.0 kJ/m²
@Temperature 23.0 °C
ISO 180/1A
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 95.0 °CISO 75-2
Flame Spread <= 100 mm/min
@Thickness 1.00 mm
ISO 3795
 
Processing PropertiesOriginal ValueComments
Melt Temperature 220 - 240 °C
Mold Temperature 20.0 - 40.0 °C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PBORE9921 / 323278

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.