MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
LyondellBasell Hifax RTA3263UV YGYA BLK Thermoplastic Olefinic Elastomer (TPO)
Categories: Polymer; Thermoplastic; Elastomer, TPE; Thermoplastic Olefinic Elastomer (TPO)

Material Notes: Hifax polypropylene resins based on the Catalloy process are used in applications such as building and construction (e.g., single-ply roofing), industrial applications (e.g., wire and cable), and automotive industries. Hifax priovides good processability, excellent impact resistance, a broad range of stiffness from very soft to rigid products, high temperature resistance and low linear coefficient of thermal expansion.

Hifax RTA3263UV YGYA BLK medium melt flow 1,600 MPa flexural modulus, paintable, mineral filled thermoplastic olefin (TPO) resin has balanced rigidity, impact strength and dimensional stability. It is typically used for rigid automotive exterior ornamentation applications requiring good weatherability. Typical applications include automotive claddings, rocker panels, license plate brackets, appliques and filler panels.

Information provided by LyondellBasell.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.09 g/ccASTM D 792
Density 1.09 g/ccASTM D 792
Melt Flow 8.0 g/10 min
@Load 2.16 kg,
Temperature 230 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 68ASTM D2240
Tensile Strength, Yield 18.0 MPaASTM D 638
Elongation at Break 40 %ASTM D638
Flexural Modulus 1600 MPaASTM D790
Gardner Impact 18.0 JASTM D5420
Tear Strength 88.0 kN/m
@Temperature -30.0 - 100 °C
ASTM D624
 
Thermal PropertiesOriginal ValueComments
CTE, linear 60.0 µm/m-°CASTM D 696
 
Descriptive Properties
Processing MethodInjection Molding

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Buckeye Polymers BP FLEX D 6509 CR Injection Grade TPO
Buckeye Polymers BP FLEX D 6020 Injection Grade TPO
Buckeye Polymers BP FLEX D 5608 T Injection Grade TPO
Buckeye Polymers BP FLEX D 5518 Injection Grade TPO
Buckeye Polymers BP FLEX D 4107 Injection Grade TPO

PEQT7279 / 218916

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.