MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Lyanchemicals Tech 803 Phenolic Resin
Categories: Polymer; Thermoplastic

Material Notes: The terpene-phenolic resin 803 and 803L, produced with rosin as the raw material, have high softening point, light color and good adhesion, and are particularly suitable for neoprene polymerization. They can be used for bonding of PVC artificial leather. Due to its they can also be applied in a variety of glue and advanced sole adhesives.

Main features: High softening point and light color; Narrow distribution of molecular weight; High bonding strength and resistance; Wide range of solubility and good phase compatibility; Extend the holding time of initial viscosity of solvent-based adhesives

Application: All solvent-based adhesives; Crafted CR adhesives; Hot melting adhesives and tapes; Senior sole adhesives, etc

Information provided by Lyanchemicals Tech Co., Ltd.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Chemical PropertiesOriginal ValueComments
Acid Value 45 - 60
 
Thermal PropertiesOriginal ValueComments
Ring & Ball Softening Point 145 - 160 °C
 
Optical PropertiesOriginal ValueComments
Gardner Color Number <= 7.0
 
Descriptive Properties
ContentPhenol

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PLYANT052 / 318079

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.