MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
Solvay RHODOLINE® 270 Surfactant
Categories: Fluid

Material Notes: Description: Polyacid dispersant. Highly versatile, economical and low foam, flat to gloss, ideal for interior application.

Identification: ACRYLIC POLYMER

CAS: 9003-04-7

Available in: North America

IR Spectrum: 0.31-0.61, RP-17642

Applications: RHODOLINE© 270 is a highly efficient anionic dispersant for pigments used in latex paints and adhesives. Use RHODOLINE© 270 at 0.6 – 1.0% (dry basis) by weight on pigment, depending upon the system. The optimum use level of RHODOLINE© 270 may be determined by the pigment dispersant demand method.

Information provided by Rhodia, Rhodia has been acquired by Solvay.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.30 - 1.33 g/ccRP-17617
Solids Content 42.8 - 43.3 %
@Temperature 130 °C,
Time 1800 sec
0.5 g; RP-0540
pH 7.0 - 8.0RP-0420
Viscosity 100 - 300 cP#2 sp @ 30 rpm; RP-0596
Molecular Weight 3400 g/mol
 
Processing PropertiesOriginal ValueComments
Shelf Life 24.0 Month
 
Descriptive Properties
AppearanceClear, Colorless to yellow liquidRP-0064

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Solvay ALKASPERSE® A-5H Surfactant
Evonik DEGAPAS® 3104 N Polyacrylate

WRHOD475 / 137706

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.