MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Evonik VESTAMID® LX9041 black 9.7504 | PA12 Nylon 12
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 12 (PA12)

Material Notes: VESTAMID® LX9041 black 9.7504 is a heat stabilized and light resistant polyamide 12 compound especially developed for extrusion coating of steel tubes. Due to the exceptional impact strength, abrasion resistance and good chemical resistance of PA 12 as well as the excellent adhesion between the steel and the properly applied VESTAMID® LX9041 black, the corrosion resistance of steel tubes coated with VESTAMID® LX9041 black is significantly increased. VESTAMID® LX9041 black is supplied as cylindrical granules, ready for processing, in moisture-proof bags.

Property data for dry samples.

Information provided by Evonik.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.02 g/ccISO 1183
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 54.0 MPaISO 527
Tensile Strength, Yield 52.0 MPaISO 527
Elongation at Break >= 50 %Nominal; ISO 527
 283 %ISO 527
Elongation at Yield 4.4 %ISO 527
Tensile Modulus 1770 MPaISO 527
50% Modulus 0.0350 GPa
@Strain 50 %
ISO 527
Flexural Strength 52.0 MPa
@Strain 7.0 %,
Temperature 23.0 °C
ISO 178
Flexural Modulus 1540 MPaISO 178
Charpy Impact, Notched 4.00 kJ/m²
@Temperature 23.0 °C
Complete Break; ISO 179/1eA
 4.30 kJ/m²
@Temperature -30.0 °C
Complete Break; ISO 179/1eA
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 9.30e+12 ohm-cmIEC 62631-3-1
Surface Resistance 2.00e+16 ohmTest specimen: platte 130x130x1mm; IEC 62631-3-2
 2.00e+16 ohmsC, circular electrodes; IEC 62631-3-2
 
Thermal PropertiesOriginal ValueComments
Melting Point 177 °CISO 11357-1/-3
Deflection Temperature at 1.8 MPa (264 psi) 48.0 °CISO 75-1/-2
Vicat Softening Point 141 °CMethod B: 10 N, 50 K/h; ISO 306
 176 °CMethod A: 10 N, 50 K/h; ISO 306
Glass Transition Temp, Tg 44.0 °CISO 11357-1/-2
Flammability Test 1.0
@Thickness 1.60 mm
IEC 60695-11-10
 1.0
@Thickness 3.20 mm
IEC 60695-11-10

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PEVONIK860 / 243068

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.