MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Dover Chemical PAROIL CW50AO Very Long Chain Chlorinated Alkane
Categories: Other Engineering Material; Additive/Filler for Polymer

Material Notes: Paroil CW50AO is a chlorinated very long chain alkane, containing a trace amount of Stabilizer to maintain product integrity during transport and storage. Paroil CW50AO is can be used as a plasticizer and flame retardant in paints, sealants, rubber, PVC and PUF. It offers water and chemical resistance for paints and coatings. Paroil CW50AO can also be used as an extreme pressure lubricant for metal working fluids. It offers low volatility and very low odor.

Information provided by DoverChem

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.219 g/cc
@Temperature 25.0 °C
Viscosity 9000 - 13000 cP
@Temperature 25.0 °C
 
Optical PropertiesOriginal ValueComments
Gardner Color Number <= 4.0
 
Component Elements PropertiesOriginal ValueComments
Chlorine, Cl 46 - 49 %
 
Descriptive Properties
Free HCl, ppm<15
Physical FormThick yellowish liquid
Stokes73-10525°C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

WDOVER077 / 217696

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.