A very common general purpose grade of medium carbon, Cr-Mo steel. Flexibility afforded by heat treatment options allows it to attain a range of toughness and strength values. Good hardenability, strength, wear resistance, toughness, and ductility. Post water quenched hardness: 51 HRC surface, 50 HRC 1/2 radius, 50 center. |
AFNOR 25 CD 4 (S), JIS SCM2, JIS SCCrM 1, SS14 2225 (Sweden), alloy steels, UNS H41300, ASTM A304, SAE J1268, DIN 1.7218, medium carbon steels, chromium-molybdenum, chrome-moly |