MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Teknor Apex TEKRON® 4300-B88 2UV Grade Thermoplastic Elastomer
Categories: Polymer; Thermoplastic; Elastomer, TPE; Thermoplastic Elastomer, Melt-Processible Rubber

Material Notes:

Information provided by Teknor Apex Company

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 0.870 - 0.910 g/ccASTM D792
Linear Mold Shrinkage 0.015 cm/cm24 hrs
 0.018 cm/cm24 hrs + 30 min. at 82°C
Melt Flow 8.7 g/10 min
@Load 2.16 kg,
Temperature 230 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 88 - 9415 second delay; ASTM D2240
Tensile Strength, Yield 1800 psiASTM D412
Elongation at Break 700 %ASTM D412
Elongation at Yield 29.5 %ASTM D412
 10 %
@Temperature -35.0 °C
ASTM D412
100% Modulus 0.860 ksi
@Strain 100 %
ASTM D412
300% Modulus 0.990 ksi
@Strain 300 %
ASTM D412
Flexural Modulus 14930 psiASTM D790
Tear Strength 56.0 pliDie C; ASTM D1004
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 47.0 °C
Flame Spread 1.28 in/minPass: Burn Rate- Max 100; FMVSS 302
 
Descriptive Properties
Fogging95.2, 6 hours at 90°C. (SAE-J1756)

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PTEKNO298 / 70041

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.