MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Overview of materials for Polyethersulfone (PES), 10% Glass Fiber Filled
Categories: Polymer; Thermoplastic; Polyethersulfone (PES); Polyethersulfone (PES), 10%Glass Fiber Filled

Material Notes: This property data is a summary of similar materials in the MatWeb database for the category "Polyethersulfone (PES), 10% Glass Fiber Filled". Specific grades with glass content between 5% and 14% are included. Each property range of values reported is minimum and maximum values of appropriate MatWeb entries. The comments report the average value, and number of data points used to calculate the average. The values are not necessarily typical of any specific grade, especially less common values and those that can be most affected by additives or processing methods.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Density 1.39 - 1.58 g/ccAverage value: 1.47 g/cc Grade Count:15
Filler Content 5.00 - 10.0 %Average value: 8.75 % Grade Count:8
Water Absorption 0.180 - 0.500 %Average value: 0.394 % Grade Count:11
Linear Mold Shrinkage 0.00100 - 0.00800 cm/cmAverage value: 0.00469 cm/cm Grade Count:15
Melt Flow 4.50 - 6.00 g/10 minAverage value: 5.00 g/10 min Grade Count:3
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 121 - 123Average value: 122 Grade Count:6
Tensile Strength, Ultimate 66.9 - 130 MPaAverage value: 102 MPa Grade Count:12
 70.0 - 95.0 MPa
@Temperature 60.0 - 150 °C
Average value: 82.5 MPa Grade Count:1
Tensile Strength, Yield 103 - 114 MPaAverage value: 109 MPa Grade Count:3
Elongation at Break 1.90 - 8.00 %Average value: 3.85 % Grade Count:15
 3.70 - 20.0 %
@Temperature 60.0 - 150 °C
Average value: 8.05 % Grade Count:1
Elongation at Yield 3.20 - 3.20 %
@Temperature 150 - 150 °C
Average value: 3.20 % Grade Count:1
Modulus of Elasticity 3.45 - 8.62 GPaAverage value: 5.27 GPa Grade Count:14
 4.10 - 4.50 GPa
@Temperature 60.0 - 150 °C
Average value: 4.33 GPa Grade Count:1
Flexural Yield Strength 121 - 179 MPaAverage value: 155 MPa Grade Count:14
Flexural Modulus 3.45 - 8.62 GPaAverage value: 5.04 GPa Grade Count:14
Compressive Yield Strength 110 MPaAverage value: 110 MPa Grade Count:3
Izod Impact, Notched 0.374 - 0.750 J/cmAverage value: 0.619 J/cm Grade Count:14
Izod Impact, Unnotched 3.74 - 11.2 J/cmAverage value: 5.94 J/cm Grade Count:8
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 1.00e+12 - 1.00e+16 ohm-cmAverage value: 7.58e+15 ohm-cm Grade Count:12
Dielectric Constant 3.70 - 4.17Average value: 3.94 Grade Count:7
Dielectric Strength 15.0 - 21.7 kV/mmAverage value: 16.7 kV/mm Grade Count:10
Dissipation Factor 0.00150 - 0.00940Average value: 0.00505 Grade Count:7
Arc Resistance 70.0 - 179 secAverage value: 120 sec Grade Count:3
 
Thermal PropertiesOriginal ValueComments
CTE, linear 25.0 - 50.4 µm/m-°CAverage value: 37.3 µm/m-°C Grade Count:8
Thermal Conductivity 0.288 W/m-KAverage value: 0.288 W/m-K Grade Count:3
Deflection Temperature at 0.46 MPa (66 psi) 207 - 220 °CAverage value: 210 °C Grade Count:5
Deflection Temperature at 1.8 MPa (264 psi) 204 - 216 °CAverage value: 209 °C Grade Count:14
Flammability, UL94 V-0Grade Count:13
 
Processing PropertiesOriginal ValueComments
Processing Temperature 343 - 366 °CAverage value: 354 °C Grade Count:3
Melt Temperature 340 - 399 °CAverage value: 363 °C Grade Count:11
Mold Temperature 120 - 177 °CAverage value: 154 °C Grade Count:13
Drying Temperature 149 - 180 °CAverage value: 155 °C Grade Count:10
Moisture Content 0.0400 %Average value: 0.0400 % Grade Count:5
Dew Point -31.7 °CAverage value: -31.7 °C Grade Count:5
Injection Pressure 68.9 - 103 MPaAverage value: 86.2 MPa Grade Count:8

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Overview of materials for Polyethersulfone (PES), 30% Glass Fiber Filled
Overview of materials for Polyethersulfone (PES), 20% Glass Fiber Filled
Overview of materials for Polyethersulfone (PES)
BASF Ultrason® E 1010 PES
Overview of materials for Polyetherimide (PEI), 30% Glass Fiber

O3711 / 78239

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.