MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Copper, UNS C62500
Categories: Metal; Nonferrous Metal; Copper Alloy

Material Notes: Good to excellent corrosion resistance. Excellent hot formability for fabrication by hot forging and machining.

Applications: guide bushings, wear strips, cams, dies, forming rolls.

Available as flat products and rod.

Key Words: CDA 625
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 7.21 g/cc
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell C 27
Tensile Strength, Ultimate 690 MPaM30 and O61 tempers
Tensile Strength, Yield 380 MPaM30 and O61 tempers
Elongation at Break 1.0 %in 50 mm, 1% reduction in area
Modulus of Elasticity 110 GPa
Compressive Yield Strength 450 MPaat permanent set of 0.1%
 880 MPaat permanent set of 1 %
Poissons Ratio 0.312
 0.312
Fatigue Strength 460 MPa
@# of Cycles 1.00e+8
M30 temper
Machinability 20 %UNS C36000 (free-cutting brass) = 100%
Shear Modulus 42.3 GPa
Izod Impact 3.00 J
@Temperature -18.0 - 100 °C
Temper not specified
Charpy Impact 3.00 J
@Temperature -18.0 - 100 °C
Keyhole
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.0000172 ohm-cm
@Temperature 20.0 °C
Magnetic Permeability 1.2
 
Thermal PropertiesOriginal ValueComments
CTE, linear 16.2 µm/m-°C
@Temperature 20.0 - 300 °C
Specific Heat Capacity 0.380 J/g-°C
Thermal Conductivity 38.9 W/m-K
@Temperature 20.0 °C
Melting Point 1047 - 1052 °C
Solidus 1047 °C
Liquidus 1052 °C
 
Processing PropertiesOriginal ValueComments
Annealing Temperature 600 - 650 °C
Hot-Working Temperature 745 - 850 °C
 
Component Elements PropertiesOriginal ValueComments
Aluminum, Al 12.5 - 13.5 %
Copper, Cu 82.7 %
Iron, Fe 3.5 - 5.0 %
Manganese, Mn <= 2.0 %
Other, total <= 0.50 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Nickel Aluminum Bronze, UNS C63200
Nickel Aluminum Bronze, UNS C63000, HR50 Temper
Chicago Extruded Metals BioBrass® UNS C62500 Aluminum Bronze
Copper, UNS C61800
Copper, UNS C61900

MC62500b1 / 11610

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.