MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
Petroquimica Triunfo Tritheva® TN 8093 EVA Copolymer  (discontinued **)
Categories: Polymer; Film; Thermoplastic; Ethylene Vinyl Acetate

Material Notes: The Tritheva TN 8093 resin is a fractional MI copolymer of Ethylene-Vinyl Acetate (EVA), developed to meet the multi-layer and blending film applications where are required high strength, with high toughness, and excellent optical properties. These packages may be produced by coextrusion and/or lamination in combination with many others materials as PVdC, PA, EVOH, etc. The resin has flexibility at low temperature that enhances applications in frozen food bags. Additionally, this resin is designed to provide a low temperature heat seal to itself or many other structure and composition commonly used in flexible packaging applications. The melt properties of this resin allow it to be processed on blow film equipments over a wide range of film thickness and blow-up ratios. Tritheva TN 8093 can be use as base polymer for the manufacture of film for greenhouses and both large and small tunnels, with excellent thermal effect at low thicknesses. This product complies with the requirements of Brazilian and corresponding legislation of Mercosul and it is in conformity with FDA Regulations 21 CFR 177.1350, to contact with foodstuff.

Applications: Food packaging (meat, cheese), coextruded heat seal layer in food packaging. High clarity film. Base polymer for agricultural film (greenhouse). Stretch hood film.

Resin Properties: Compressed molded plate. Method ASTM D-1928, procedure C. Film obtained on a 50mm blow film line with barrier screw, 25:1 L/D, 1.0mm die gap, 50µm gauge, 2.3:1 BUR.

Information provided by Dax Resinas

Petroquimica Triunfo has been acquired by Braskem.

Key Words: FDA: 21 CFR 177.1350
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.934 g/ccASTM D1505
Vinyl Acetate Content 11 - 13 %
Thickness 50.0 microns
Melt Index of Compound 0.30 - 0.50 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 26.0 MPaASTM D638
Tensile Strength, Yield 5.00 MPaASTM D638
Film Elongation at Break, MD 460 %ASTM D882
Film Elongation at Break, TD 760 %ASTM D882
Elongation at Break 660 %ASTM D638
Secant Modulus, MD 0.0530 GPa5%; ASTM D882
Secant Modulus, TD 0.0550 GPa5%; ASTM D882
Elmendorf Tear Strength, MD 28.0 g/micronASTM D1922
Elmendorf Tear Strength, TD 5.90 g/micronASTM D1922
Dart Drop Test 425 g(method A); ASTM D1709
Film Tensile Strength at Break, MD 32.0 MPaASTM D882
Film Tensile Strength at Break, TD 33.0 MPaASTM D882
 
Thermal PropertiesOriginal ValueComments
Melting Point 96.0 °CASTM D3418
 
Optical PropertiesOriginal ValueComments
Haze 1.7 %ASTM D1003
Gloss 132 %@ 60° Gardner; ASTM D2457
 
Processing PropertiesOriginal ValueComments
Processing Temperature 140 - 155 °CPlasticizing Zone
 155 - 170 °CMixture Zone
Feed Temperature 140 - 150 °C
Adapter Temperature 170 - 190 °C
Blow-up Ratio (BUR) 3.0Recommended
 
Compliance PropertiesOriginal ValueComments
FDA YesSee notes for details.

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Petroquimica Triunfo Tritheva® PN 2021 EVA Copolymer
Celanese Ateva® 1880A Ethylene Vinyl Acetate Copolymer
Eurofoam Evacell EVA 50/S EVA + NR Foam
Arkema OREVAC® 9309 EVA Terpolymer
Braskem VA2019A EVA Foam Copolymer

PDAX115 / 29540

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.