MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
CIMBAR Suspengel™ 200 Plus High Purity Bentonite, Industrial Grade
Categories: Ceramic; Clay; Oxide; Silicon Oxide; Other Engineering Material; Additive/Filler for Polymer

Material Notes: Suspengel products are manufactured from the highest quality Western Bentonite reserves. Suspengel products are easy to disperse thixotropes with excellent suspension properties. Strict process control assures our customers of the most consistent products on the market.

Typical Industrial Uses:

  • Agricultural Products - Pesticides, Fertilizers, Fungicides
  • Coatings Market - Rheological additive, Suspension
  • Paper Industry - Suspension, De-Inking
  • Industrial Markets - Ceramics, Adhesives, Caulks, Sealants, Foundry/Refractory
  • Environmental Applications - Water Treatment, Waste Treatment, Pond/Lake Sealing

Information provided by Cimbar Performance Minerals.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 2.50 g/cc
Bulk Density 72.0 lb/ft³
Oil Absorption 34 %g oil/100 g filler; ASTM D281-31
Moisture Absorption at Equilibrium 8.0 %
Loss On Ignition 14 %
Particle Mesh Size 200 Mesh80.0% passing, dry
 200 Mesh98.0% passing, wet
 325 Mesh95.0% passing, wet
pH 9.0
Viscosity 18 cPApparent
Viscosity Measurement 12Plastic Viscosity (FV)
 
Component Elements PropertiesOriginal ValueComments
Al2O3 21.4 %
CaO <= 0.60 %
Fe2O3 3.8 %
K2O 0.30 %
MgO 2.3 %
Na2O 2.5 %
SiO2 63.3 %
 
Descriptive Properties
Base Exchange Capacity (meq/kg)98
Surface Area N2 Absorption (m²/g)20
Yield Point (Lb/100 ft²)16

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
COI Ceramics Sylramic™ Crystalline Silicon Carbide (SiC) Fiber
COI Ceramics Nextel™ AS-N312 Oxide Ceramic Matrix Composite, Aluminosilicate
Clay, Soft Shale
CIMBAR Suspengel™ 16 High Purity Bentonite, Industrial Grade
Chosun Refractories SBN-1 Bricks, Reaction Bonded SiC

CIMBAR961 / 133443

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.