MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
FKuR Kunststoff Biograde® C 5508 Cellulose Acetate
Categories: Polymer; Renewable/Recycled Polymer; Thermoplastic; Cellulosic; Cellulose Acetate, Molded

Material Notes: Biograde® C 5508 is a slightly yellowish and translucent cellulose compound for injection molding. It contains a high amount of renewable resources and has a Biobased Carbon Content of more than 60%. The cellulose used for this compound is derived from wood from sustainable forestry, no tropical woods are used. The raw materials are not of animal origin and also not genetically modified. Biograde® C 5508 can be used on standard injection molding machinery with standard screws and performs in multi-cavity moulds and does not need special screw designs. This compound can be easily colored and is suited for the contact with food. Biodegradable compound for injection molding made partially from biobased resources.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.27 g/ccISO 1183
Linear Mold Shrinkage 0.0039 - 0.0085 cm/cmISO 294-4
Melt Flow 18 - 25 g/10 min
@Load 5.00 kg,
Temperature 230 °C
ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Ultimate 53.0 MPaISO 527
Tensile Strength, Yield 55.0 MPaISO 527
Tensile Modulus 2460 MPaISO 527
Flexural Strength 62.0 MPa
@Strain 3.5 %
ISO 178
Flexural Modulus 2620 MPaISO 178
Charpy Impact Unnotched NB
@Temperature 23.0 °C
ISO 179-1/1 eU
Charpy Impact, Notched 10.5 kJ/m²
@Temperature 23.0 °C
ISO 179-1/1 eA
 
Thermal PropertiesOriginal ValueComments
Melting Point >= 180 °CISO 3146-C
Vicat Softening Point 107 °CISO 306
 
Descriptive Properties
Bio-based carbon content (%)60ASTM D 6866

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PFKUR910 / 192730

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.